Solvay to Buy Gharda's Specialty Polymers

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon

Solvay SA of Belgium, parent of Solvay Advanced Polymers, Alpharetta, Ga., announced a deal to acquire the Polymer Div. of Gharda Chemicals in India.

Solvay SA of Belgium, parent of Solvay Advanced Polymers, Alpharetta, Ga., announced a deal to acquire the Polymer Div. of Gharda Chemicals in India. Gharda Polymers, which has a sales office in Newtown, Pa., produces PEEK and other polyketones, polysulfone, polyethersulfone, and polyphenylsulfone—all also made by Solvay.