Molder of Large Totes Save Material & Energy Costs with Recycled PP
Aaron Industries’ 100% recycled PP compound fortified with Milliken’s specialty modifier boosts MFI and retains strength.
A manufacturer of specialty recycled thermoplastic compounds, Aaron Industries Corp. in Leominster, Mass., is winning praise from customers who make housewares with the recent launch of its Jet-Flo Polypro high-melt-flow compound. Not only does the recycled PP compound promote sustainability but it allows for molding thinner, lighter parts that require both less material and energy.
The “secret sauce” in this new compound is a DeltaMax Performance Modifier from Milliken & Co.. Spartanburg, S.C., part of a new additive line joining the company’s well-known clarifiers and nucleating agents. As previously reported, Milliken describes this family of products as novel reactive extrusion modifiers, which reportedly maximize PP impact strength and MFI without compromising stiffness (see June ’18 feature). These improved properties allow PP to be used in a wider range of applications in more cost-effective ways. In addition to being tailored for use in impact PP copolymers, DeltaMax technology has also proven effective in modifying post-consumer and post-industrial recycled resins. It elevates impact and melt flow to the same level as—or better than—those of virgin resin, a capability that allows compounders and converters to use up to 100% recycled PP without sacrificing performance or processing.
Robert Tocci, v.p. of Aaron Industries says the new Jet-Flo Polypro is among the first recycled PP materials to combine two properties that are normally mutually exclusive: extremely high MFI of 50-70 g/10 min and good impact performance (notched Izod of 1.5-2.0 ft-lb/in). High MFI and good toughness suit this compound to economical, highly durable, thin-wall parts, such as housewares. By adding significant value to recycled PP, Aaron Industries is helping to encourage broader use of sustainable alternatives to virgin PP resin.
According to Tocci, Aaron Industries historically has used peroxide to increase the MFI of its recycled PP, but that method reduces impact strength. This led the company to work with Milliken and its DeltaMax modifiers, which reportedly can increase MFI up to fivefold while maintaining impact strength. The two companies finalized the development of the Jet-Flo compound, which is available as gray and black pellets in eastern parts of the U.S. and Canada.
Notes Tocci, “We started by doing a lot of internal testing as we have a full-scale lab.” This followed field testing with two molders of 20-30 gal PP totes. “This DeltaMax modifier has a really high upside. These molders have been transitioning to very-high-melt-flow PP—from 20-30 MFI to 50, 60 and 80 MFI--as they want to produce these totes with thinner walls and save money. This is a very high-volume market, and we couldn’t make an entry with a repro compound because we didn’t have an additive that would both increase the MFI and maintain impact strength.”
Not only does Milliken’s DeltaMax enable Aaron’s 100% post-industrial recycled PP compounds to achieve the desired blend of MFI and toughness, but a molder making a 20-gal tote reportedly can reduce molding temperatures by 20-30º F and can run bigger molds on a smaller machine. “We’ve seen cycle-time reduction of 5-15% depending on molding temperature,” says Tocci. The DeltaMax fortified compound allows for more complex and thinner-wall geometries for products ranging from housewares and lawn/garden products to automotive components.
Related Content
Improving Twin-Screw Compounding of Reinforced Polyolefins
Compounders face a number of processing challenges when incorporating a high loading of low-bulk-density mineral filler into polyolefins. Here are some possible solutions.
Read MoreDensity & Molecular Weight in Polyethylene
This so-called 'commodity' material is actually quite complex, making selecting the right type a challenge.
Read MorePolyethylene Fundamentals – Part 4: Failed HDPE Case Study
Injection molders of small fuel tanks learned the hard way that a very small difference in density—0.6%—could make a large difference in PE stress-crack resistance.
Read MoreFormulating LLDPE/LDPE Blends For Abuse–Resistant Blown Film
A new study shows how the type and amount of LDPE in blends with LLDPE affect the processing and strength/toughness properties of blown film. Data are shown for both LDPE-rich and LLDPE-rich blends.
Read MoreRead Next
How Polymer Melts in Single-Screw Extruders
Understanding how polymer melts in a single-screw extruder could help you optimize your screw design to eliminate defect-causing solid polymer fragments.
Read MoreUnderstanding Melting in Single-Screw Extruders
You can better visualize the melting process by “flipping” the observation point so that the barrel appears to be turning clockwise around a stationary screw.
Read MoreTroubleshooting Screw and Barrel Wear in Extrusion
Extruder screws and barrels will wear over time. If you are seeing a reduction in specific rate and higher discharge temperatures, wear is the likely culprit.
Read More