Plastics Processing Expands in July
With an Index reading of 52.3, processors report first monthly expansion since the coronavirus disruption.
The Gardner Business Index (GBI) for plastics processors—based on monthly surveys of Plastics Technology subscribers—reported its first expansionary reading in July, coming in at 52.3, while the nation and economy continue to battle the spread of the novel coronavirus. Survey results provided by custom processors in particular also revealed better business conditions (Fig. 1).
Among the components that constitute the overall index, new orders and production both showed expanding activity in July vs. June (Fig. 2). All index components had higher readings in absolute terms for the month, with exports and backlogs reporting quickly slowing decline in their respective areas of activity.
FIG 1 Both the overall and custom processor indices reported expanding business activity in July for the first time since COVID’s severe disruption of the economy.
The greater than nine-point gain in the index for new orders was not only the highest since April 2019, but indicated expanding order activity for the first time while the economy operates under the shadow of COVID-19. Historically, new orders have acted as a bellwether for other components of the index, including production, backlogs and employment. Should new orders continue to experience expanding activity in future months, it would be reasonable to expect these other measures of business activity to expand too. Simultaneously, the industry continues to signal that supply chains remain severely disrupted; this may delay the return of normal production levels and hiring.
FIG 2 New orders and production reported their first month of slowing decline in July after a sharp drop in June.
Editor’s Note: The Plastics Processing Business Index is unique in its ability to measure business conditions specific to plastics processors on a monthly basis. The challenges facing manufacturers today require leaders to have good data in order to make effective forward-looking decisions. It is particularly important at this time for our readers to complete the survey sent to them each month. Your participation will enable the best and most accurate reporting of the true impact that COVID-19 is having on the plastics industry.
If you are a North American plastics processor and would like to participate in this research, click here to begin the process by subscribing free to Plastics Technology magazine.
About the Author: Michael Guckes is chief economist and director of analytics for Gardner Intelligence, a division of Gardner Business Media, Cincinnati. He has performed economic analysis, modeling, and forecasting work for more than 20 years among a wide range of industries. He received his BA in political science and economics from Kenyon College and his MBA from Ohio State University. Contact: (513) 527-8800; mguckes@gardnerweb.com.
Related Content
-
50 Years...600 Issues...and Still Counting
Matt Naitove marks his first half-century in plastics reporting, with a few of his favorite headlines.
-
Mold Opaque White PET Bottles – Without Pigment
Trexel and Husky are cooperating on molding recyclable opaque white preforms for PET bottles, which provide a light barrier using foam instead of pigment.
-
How Inline Vision Inspection Can Minimize Scrap in Molding
Once viewed by injection and blow molders as a necessary evil, machine vision technology today can continuously monitor and improve production while reducing costs.