3D Printing LSR
Yes, you read that right: Liquid silicone rubber (LSR) is 3D printable.
At NPE2018 in Orlando, Fla., Distributor RDAbbott, Cerritos, Calif., showed off a system for 3D printing with LSR, developed by Dow Silicones (previously Dow Corning), Midland, Mich., and German RepRap, a maker of 3D printing equipment.
Called Liquid Additive Manufacturing (LAM), the system injects liquid A and B components from two pressurized tubes into a pump that maintains a 1:1 ratio. The pump feeds a head under x-y motion control, which and lays down a continuous bead, similar to FDM or FFF-style 3D printers. The system deposits layers as thin as 0.2 to 0. 35 mm thick, which are fully cured by a heat lamp, a whole layer at a time. The system uses Dow’s Evolv3D LC 3335 LSR material, which produces a 44 Shore A hardness without post-cure and 46A with post-cure. The LAM 3D printer reportedly produces parts with 100% of the tear strength of injection molded samples, 90% of their tensile strength and hardness, and 85% of their elongation. Applications in development include honeycomb custom orthotic shoe soles.
The patent-pending printer was introduced last year; it can print at 10 to 150 mm/sec, depending on the geometry. Dow is developing additional LSR grades, expected later in the year, that will offer other Shore A hardnesses.
Though remarkable, this is not the first 3D printing system for LSR. The German parent of Wacker Chemical Corp., Adrian, Mich., introduced the ACEO system of hardware and LSR materials for 3D printing in 2016 (see our K 2016 report in Feb. ’17).
Related Content
-
Large-Format “Cold” 3D Printing With Polypropylene and Polyethylene
Israeli startup Largix has developed a production solution that can 3D print PP and PE without melting them. Its first test? Custom tanks for chemical storage.
-
Freeform Injection Molding Eases the Path to Medical Device Product Testing
A development and manufacturing service provider is using dissolvable molds to build injection molded silicone prototypes.
-
Getting into Plastics Additive Manufacturing? Avoid these Six Common Errors
There are a lot of 3D printing technologies out there, and it’s not uncommon for processors new to additive manufacturing to get tripped up. Here are some typical snafus, along with advice on how to avoid them before you start making parts.