All-rPET Bottles with Glued-in Handles Save Material
At K 2022, KHS is showing a 2.3 L PET bottle with glued-in handle that offers 10% material savings and other advantages over clip-in handles. Bottle and handle are both 100% rPET.
Energy savings, greater design freedom, high clarity and lack of seams are advantages claimed by KHS for its new 2.3 L rPET bottle with glued-in handle vs. PET with clip-in handle or extrusion blown polyolefin handleware. (Photo: KHS)
KHS has a new option for stretch-blown PET containers with handles: Besides offering clip-in handles slotted into place mechanically, KHS is exhibiting at K 2022 a new 2.3-liter PET bottle with a glued-in handle. Both bottle and handle are 100% rPET. The company says this design, together with the preferential heating technology on its stretch-blow machines, provides 10% material savings vs. bottles with clip-in handles. Glued-in handles reportedly also require a simpler contour and increase efficiency in processing.
In addition, the clear PET bottle has a marketing advantage over translucent extrusion blow molded HDPE or PP handleware. And the lack of seams in the stretch-blown PET bottle reportedly contributes to excellent performance in rigorous drop tests.
The new bottle results from an 18-month cooperative project between KHS and Logoplaste Innovation Lab, a division of the Portugal-based Logoplaste Group, which has 63 bottle-making plants in 17 countries. It’s three Innovation Hubs are located in Portugal, U.K. and Plainfield, Ill. The goal of the project was to design a bottle for home-care products with the smallest possible carbon footprint. The project drew on KHS’s experience in selecting a suitable adhesive from prior projects.
Related Content
-
New Technology Bonds Aluminum With Polyamides
With many benefits for numerous potential applications, including in the burgeoning electric vehicle market, Celanese’s Zytel Bonding Technology achieves stronger bonds than overmolding or welding.
-
New Designs for Electric & Hybrid Packaging and Industrial Blow Molding Machines
Introduced at K 2022, Bekum’s 21 models in the new EBLOW 8 Series and XBLOW designs include all-electric packaging machines from small to large, plus industrial units with a novel two-stage clamp in servohydraulic or hybrid versions.
-
Energy Efficiency in Focus at K 2022
As much as cycle time, kWh/kg was an oft-cited metric by injection molding machine suppliers at October’s big show.