Extrusion: Software Simulates Extrudate Cooling and Shrinkage
Eliminates need for processors to purchase two separate software packages for simulating the flow inside the die and for predicting the extrudate cooling.
The new version of Plastic Flow’s polyXtrue software allows users to accurately simulate extrudate cooling and corresponding extrudate shrinkage. This means there is no need for processors to purchase two separate software packages for simulating the flow inside the die and for predicting the extrudate cooling.
The new version now includes the effect of shrinkage due to extrudate cooling as well as the effect of non-uniform exit velocity to accurately predict the extrudate distortion and the shape of the final extruded product.
For an accurate analysis of extrudate cooling, shrinkage, and distortion, the new version of polyXtrue starts by treating the polymer as a melt near the die exit, but then transforms the analysis to treat the extrudate as a solid at lower temperatures away from the exit. This unified fluid-solid analysis of extrudate gives an unprecedented accuracy in the predicted temperature and distortion of the extrudate. The algorithm for the post-die analysis has been completely revamped to simulate this coupled fluid-solid system while also improving the computational speed of the software. Furthermore, the flow in the calibrator as well as in the post-calibrator region is included in the analysis.
Users can continue to run the latest release as an add-in inside SolidWorks and Inventor. The optiXtrue software then allows you to automatically optimize your extrusion dies by parameterizing the critical die dimensions in either of the two geometric modeling software packages. Many of the other important features from the previous versions of polyXtrue, such as accurate prediction of layer structure in the final product; accelerated computation speed using the Graphics Processing Unit (GPU) of your computer have been further improved in the new version.
The graphical user interface (GUI) of the software has also been updated with a large number of new features to make the software more effective and even more user friendly.
This release of polyXtrue is also available as the Pay-Per-eXecution (PPX) version. The free PPX version of polyXtrue can be downloaded here.
Related Content
-
High-Speed Cutters for Corrugated Tubing
Applications for new cutter line include medical, automotive, and other industrial.
-
Online X-Ray Inspection Boosts Extrusion Quality
Höhle uses Sikora’s x-ray measuring systems for inline quality control of extruded microducts.
-
How to Effectively Reduce Costs with Smart Auxiliaries Technology
As drying, blending and conveying technologies grow more sophisticated, they offer processors great opportunities to reduce cost through better energy efficiency, smaller equipment footprints, reduced scrap and quicker changeovers. Increased throughput and better utilization of primary processing equipment and manpower are the results.