ADDITIVES: High-Performance Stabilizers for Polyolefins in Outdoor Use

Solvay's Cyasorb Cynergy B Series stabilizers aimed at outdoor building & constructions applications.

Related Topics:

Related Suppliers

A new line of stabilizers said to deliver exceptional UV and long-term thermal stability to PP and other polyolefin parts used in outdoor building and construction applications has been added to the proprietary Cyasorb Cynergy Solutions portfolio of Solvay Technology Solutions, Woodland Park, N.J. (formerly Cytec Industries).

            The new B Series stabilizers are suitable for use with neat and reinforced thermoplastics, and reportedly will not contribute to blooming or delamination in painted parts. Specific applications targeted include TPO roofing, polyolefin roofing tiles, polyolefin roofing shakes, solar shingles, siding, shutters, and geomembranes. 

Editor Pick

A Gel By Any Other Name...

Gels…unmelt…contaminants…inclusions…whatever you call them, you want to avoid them. Proper maintenance and good housekeeping—lids on boxes, closed hopper doors, core-free reclaim systems—go a long way towards defect-free product.