EconCore and MEAF Partner in Specialized Lab Extruder Development
Check the latest in EconCore’s progress in the development of new all-thermoplastic continuous honeycomb cores.
In late March, I blogged about Belgium’s EconCore’s extended capabilities of its ThermHex technology to produce continuous honeycombs from several high-performance thermoplastics. Now the company has partnered with Holland’s MEAF Machines to develop and install a fully-functional laboratory-scale extrusion and forming line at the company’s recently-refurbished R&D facilities in Leuven, Belgium.
At the heart of the line is a purpose-built 50-mm extruder equipped with a special 500-mm sheet die built by Austrian flat-die specialist EMO Extrusion Molding. EconCore patented ThermHex technology produces honeycomb structures from a single continuous thermoplastic sheet. This involves a sequence of thermoforming, folding and bonding operations.
Cell size, density and thickness of the honeycombs can be altered with simple hardware and/or process parameter adjustments. The process allows for inline bonding of solid skins to one or both sides of the honeycomb, to create an extremely cost-effective finished composite panel.
Prior to the installation of the new purpose-built extruder, EconCore was carrying out its honeycomb developments using sheet unwound from a roll. “Now that we can produce our own sheet in-line, we have more flexibility in our operations and it is obviously much easier to make changes to the material formulations,” says technical manager Wouter Winant. EconCore and MEAF collaborated closely on the design of the laboratory extruder, which is equally capable of processing polyolefins, bioplastics and high-performance thermoplastics such as PC, nylons and PPS.
Explains Winant, “This is a non-typical set-up, but it is very important for our development work. EconCore already has licensees around the world producing continuous honeycombs and honeycomb-cored laminates in polyolefins—predominantly polypropylene—and we intend to continue refining the process technology for these materials. The new line is partly intended for this purpose. At the same time though, we are extending the potential of ThermHex technology by enabling it to be used with thermoplastics with superior mechanical and thermal performance—what we call HPTs. Normally this would require the use of a second extruder, since the processing characteristics of polyolefins are quite different from those of HPTs. But with this purpose-designed extruder, we have so far managed to obtain excellent results on around 10 different kinds of polymers.”
The MEAF extruder has a 50-mm barrel holding a screw with an L:D of 34:1, which is typical for polyolefins. However, it also has a superior heating capability, with each of its five zones rated at 5.8 kW. Despite this high-power rating, the extruder is highly energy-efficient, in line with MEAF’s philosophy of creating extrusion systems with low carbon footprints. A 600-L dryer for hygroscopic materials is fully integrated into the production system. Maximum output from the extruder is around 150 kg/hr.
“We have been cooperating with MEAF for several years now, on various projects, and the results have always been very encouraging. Both our companies are small/medium-sized, with a flexible approach to getting things done, and a strong thirst for success, so we work together well,” says EconoCore’s COO Tomasz Czarnecki,
Czarnecki notes that licensees of the company’s ThermHex process have no obligation to use MEAF extruders, but often tend to decide to choose this option, as they are encouraged when seeing the results this equipment delivers. Adds Czarnecki, “The call for innovative, light-weighting material solutions is very loud while the cost-efficient processing within the integrated production process combined with cost savings linked to the product’s weight reduction and production energy-efficiency is at high demand. This generates the fuel for our developments. After successful commercial evolutions within the current, globally distributed network of our licensees in the sectors of industrial packaging, building, automotive as well as wider transportation and others, and with the new, exciting license projects in the pipeline, we intend to continue our cooperation to take ThermHex technology to the next level, amongst others with HPTs.”
Related Content
Automation in Thermoforming on the Rise
Equipment suppliers’ latest innovations exemplify this trend driven by factors such as labor shortages, higher-speed thermoformers and tighter quality control.
Read MoreUS Merchants Makes its Mark in Injection Molding
In less than a decade in injection molding, US Merchants has acquired hundreds of machines spread across facilities in California, Texas, Virginia and Arizona, with even more growth coming.
Read MoreHigh-Temperature Syntactic Foam and High-Slip Plug Materials for Thermoforming
At K 2022, CMT Materials to launch new Hytac syntactic foam and a developmental higher slip plug materials with no PTFE.
Read MoreBrueckner Group USA Moving to Bigger Space
New facility in New Hampshire will serve the local customer base better and enhance capabilities in the North American market.
Read MoreRead Next
Advanced Recycling: Beyond Pyrolysis
Consumer-product brand owners increasingly see advanced chemical recycling as a necessary complement to mechanical recycling if they are to meet ambitious goals for a circular economy in the next decade. Dozens of technology providers are developing new technologies to overcome the limitations of existing pyrolysis methods and to commercialize various alternative approaches to chemical recycling of plastics.
Read MoreProcessor Turns to AI to Help Keep Machines Humming
At captive processor McConkey, a new generation of artificial intelligence models, highlighted by ChatGPT, is helping it wade through the shortage of skilled labor and keep its production lines churning out good parts.
Read MorePeople 4.0 – How to Get Buy-In from Your Staff for Industry 4.0 Systems
Implementing a production monitoring system as the foundation of a ‘smart factory’ is about integrating people with new technology as much as it is about integrating machines and computers. Here are tips from a company that has gone through the process.
Read More