A new long-fiber polypropylene concentrate contains 80% glass loading by weight-reportedly the highest long-fiber content available.

Related Suppliers

A new long-fiber polypropylene concentrate contains 80% glass loading by weight-reportedly the highest long-fiber content available. RTP Co., Winona, Minn., says the high loading decreases the amount of concentrate required during blending, which reduces cost for the processor.