MATERIALS: Acrylic-Based Liquid Thermoplastics Process Like Thermosets

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon

Arkema's liquid thermoplastics are based on a high-molecular-weight acrylic and can be transformed using the same processes as composite thermosets.

Share

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon

Related Suppliers

The first range of a new family of liquid thermoplastics that are transformed via reactive closed-mold processes such as room-temperature infusion, RTM, and flex-molding as used with composite thermosets have been introduced by Arkema (U.S. office in King of Prussia, Penn.). Elium resins boast quick polymerization and can be used to design structural parts as well as aesthetic elements in the automotive, transportation, wind power, sports and building and construction industries.

Arkema formulated these novel resins based on a high-molecular-weight acrylic polymer under peroxide initiated radical polymerization, using the company’s Luperox organic peroxide which was specifically developed for this purpose, according to product manager Sebastien Taillemite. Composite parts made from Elium are 30-50% lighter than their steel counterparts, but offer the same resistance.  Such parts cost less to manufacture than other thermoplastic composite technologies: they are said to be easy to use in thermoset processes, transform at room temperature, and do not contain any fabricated products like organo-sheets. Elium resins have a range of reactivity based on the grade. Certain grades have been optimized for elevated temperature curing in a matter of minutes to room temperature with part cycle times ranging from 20 min. to a few hours depending on the part size and process.

Says Taillemite, “The technology allows us to obtain a thermoplastic polymer that is recyclable, weldable and thermoformable at 200-220 C (392-428 F), and its high molecular weight results in mechanical properties that are excellent and enable the manufacture of structural parts with both carbon fiber and glass fiber, when the correct sizing is used.” He gives the example of Arkema’s collaboration with Belgium fiberglass producer 3B to develop a specific glass fiber sizing that enhances matrix-fiber adhesion.  At this stage, Elium has been brought to the level of epoxies with respect to mechanical properties, but with much higher toughness than epoxies and no need for post-curing to reach the glass transition temperature (Tg). The company has customers who have made very different parts from Elium, from boat hulls to vehicle parts, and also most recently a wind blade. Traditional plastics processing equipment can be utilized in the reprocessing of recycled and reclaimed material.

(800) 225-7788 • www.arkema.com

RELATED CONTENT

  • The New Lightweights: Injection Molded 'Hybrid' Composites Spur Auto Innovation

    A thermoplastic composite technology that emerged just a couple of years ago promises to make dramatic strides within the next two years in automotive mass production of structural components.

  • Melt Flow Rate Testing–Part 1

    Though often criticized, MFR is a very good gauge of the relative average molecular weight of the polymer. Since molecular weight (MW) is the driving force behind performance in polymers, it turns out to be a very useful number.

  • Thermoplastic Polyesters: It's Time to Know Them Better

    There’s more to TP polyesters than you think. You may know PET, PBT, and PETG—but what about PCT, PCTG, PCTA, and PTT? If you’re not sure what they are, how their properties compare, and who sells them, we have the answers—and lots of new developments to report.

Resources