WEB EXCLUSIVE Lectro Engineering Co., St. Louis, Mo., has boosted the capacity of its 3D open-air plasma-discharge system by 50% over previous models. The new LT 2012 Plastics Surface Treater for molded parts also has a 65% smaller footprint than the LT 2000 Series. The higher capacity is said to open up new applications in areas like automotive that are seeking more environmentally friendly adhesion promoters. The smaller footprint was made possible by reconfiguring the high-voltage system. (314) 567-3100 * www.lectrotreat.com