'Plug-and-Play' Bioplastic Platform Results in Various Grades of PC
Teysha Technologies' proprietary platform enables development of polymers that combine strength and toughness with hydrolytic breakdown to biologically beneficial byproducts at end of life.
We recently were contacted by U.K.-based Teysha Technologies, which after more than a decade of research has achieved a landmark breakthrough in creating a viable substitute for existing petroleum-based PC resins, and potentially other plastics
Explains project research scientist Ashlee A. Jahnke, “Our technology uses a plug-and-play system that takes monomers and co-monomers—the natural building blocks that make up plastic—to create a polymer that works and functions in a very similar way to the plastic we’re used to. The difference is that our monomer feedstocks are derived from natural sources such as starches and agricultural waste products, rather than hydrocarbon-based petrochemicals sourced from fossil fuels.”
Moreover, the platform the researchers have created to build these biopolymers reportedly allows them to precisely tune the physical, mechanical and chemical properties of the resulting polymer to make it usable in a variety of materials. As such, they are able to adjust the strength, toughness, durability and longevity of the polymers to suit different applications. Says Jahnke, “We can create rigid or flexible materials, or ones that offer different thermal properties. Crucially, we can also control the biodegradation of our polymers so that they breakdown in weeks or years, returning back to their basic building blocks that can be beneficial to plants.”
Here are Jahnke’s responses on some key questions we posed regarding the status of the technology:
● Does your technology result in a PC type polymer only at this juncture? When you say it can produce a wide range of plastics, does it mean different grades of PC and/or PC blends... or other thermoplastics?
“Currently, all the plastics we produce are polycarbonates, but many also contain ester bonds. We can also produce simple polyesters using our technology platform. We can produce a wide range of plastics because our plug-and-play platform allows us to use various natural product monomers as polymer building blocks, and our current focus is on various grades of polycarbonate.”
● Are you licensing the technology? Globally?
“We are not licensing at the moment, but we will be exploring several commercial arrangements, both upstream and downstream, and global licensing will most definitely form part of our strategy. Our chairman, Dr. Clive Rankin, has particular experience in this field as ex-vice president of Degussa Fine Chemicals.”
● Is there any performance data you can share comparing the material to virgin PC and/or other bio-based plastics like PLA?
“We don't have much of this type of direct comparison data at this point, but this is something that we are working on. We do know that our degradation temperatures are comparable to other bioplastics, and a bit lower than typical PC on the market. Other performance characterization work is ongoing.”
● Is anyone using the technology toward a commercial end? Are these polymers for injection molding? Extrusion? Blow molding? Is it for rigid products or flexible products as well? Can you list potential applications?
“The technology is not yet at the commercial stage. However, our thermoset polymers have demonstrated the ability to be molded and cured, by both UV and heat, to form prototype fishing lures. The thermoplastics will likely be best for injection molding, but we have not begun testing this yet.
“Beyond these applications, our technology platform allows us to be very versatile, because the products can be either rigid or flexible depending on the monomers used for polymerization. As such, there is a wide range of potential applications, from building insulation to food packaging and medical implants to drug delivery systems. We have even considered molding for automobiles.”
Related Content
PEEK for Monolayer E-Motor Magnet Wire Insulation
Solvay’s KetaSpire KT-857 PEEK extrusion compound eliminates adhesion and sustainability constraints of conventional PEEK or enamel insulation processes.
Read MoreDesign Optimization Software Finds Weight-Saving Solutions Outside the Traditional Realm
Resin supplier Celanese turned to startup Rafinex and its Möbius software to optimize the design for an engine bracket, ultimately reducing weight by 25% while maintaining mechanical performance and function.
Read MoreHonda Now Exploring UBQ’s Biobased Material Made from Unsorted Household Waste
UBQ is aiming to expand its reach for more sustainable automotive parts as well as non-automotive applications.
Read MoreNew Technology Bonds Aluminum With Polyamides
With many benefits for numerous potential applications, including in the burgeoning electric vehicle market, Celanese’s Zytel Bonding Technology achieves stronger bonds than overmolding or welding.
Read MoreRead Next
Understanding Melting in Single-Screw Extruders
You can better visualize the melting process by “flipping” the observation point so that the barrel appears to be turning clockwise around a stationary screw.
Read MoreLead the Conversation, Change the Conversation
Coverage of single-use plastics can be both misleading and demoralizing. Here are 10 tips for changing the perception of the plastics industry at your company and in your community.
Read MorePeople 4.0 – How to Get Buy-In from Your Staff for Industry 4.0 Systems
Implementing a production monitoring system as the foundation of a ‘smart factory’ is about integrating people with new technology as much as it is about integrating machines and computers. Here are tips from a company that has gone through the process.
Read More