Worldwide Switch to New Gauging System Pays Off for Haartz
Leading supplier of sheet and roll stock for automotive applications reevaluated its thickness-measurement technology in 2012, and now has 15 scanners in place worldwide from one supplier.
Family owned and in business more than 100 years, Haartz Corp., Acton, Mass., is the world’s leading supplier of automotive topping fabrics and a leading producer of soft-trim car interior materials. Roll and sheet goods made by Haartz can be found in almost every automotive brand worldwide, especially in convertible tops.
In Acton, surface effects such as simulated leather are embossed into extruded PVC, TPO or other compounds to create formable and hand-wrap materials. These materials are used in door panels, seats, console lids, instrument panels, and more for automakers from Nissan to BMW. Some lines are set up to extrude material onto a thin layer of foam, giving the trim more cushion. Haartz also extrudes plastic between two layers of fabric.
In 2012, an effort to streamline production focused on the company’s web gauging and control systems. “Back then, our web scanners were made by two well-known manufacturers,” recalls John Gilbert, senior process engineer in Acton. “Our people wanted to find the best scanner brand for us as we began planning the upgrade of our extrusion lamination lines.”
Haartz typically runs at thicknesses ranging from 0.5 to 1.3 mm. Strict control of the extrusion process is critical to meeting Tier 1 supplier specs as well as IATF16949 Automotive Quality standards. Going outside standard deviation limits risks failing spec and wasting material. So, by employing just one brand of gauging system across the board, Haartz could enable all line operators to gain a better knowledge of the system selected and produce more consistent and efficient products.
“Because we run the lines on a 24/5 or 24/6 basis, our operators need to move from line to line so vacations, sick days, and shift changes can be well covered,” Gilbert said. “It was crucial to select a system they all could easily adapt to and that could fulfill all our requirements as we pushed our capability.”
KICKING ALL THE TIRES
The company wanted the best system for its future. “We talked with every major manufacturer out there,” Gilbert explains. “Our search included a parade of presentations and proposals, plus dozens of site visits over many months and several states.”
What they learned surprised everyone on the selection team. One brand not only fit all their needs, but Haartz found the differences between a system provided by Mahlo America, Spartanburg, S.C. (mahloamerica.com) those from all other vendors were “stunning.” The team’s first impression was that the machine “is built like a tank.” As a bonus, most Mahlo parts are easily sourced from aftermarket suppliers--even motors and circuit boards. “With our legacy scanners we were compelled to sign service contracts,” Gilbert admits. “After X number of years, the manufacturers stop supporting them. We were expected to buy new.”
Gilbert adds, “Mahlo said they still support scanners 25 and 30 years old. That moved them to our short list.” Still, changing control systems is a challenge. Change can cause people to fear making mistakes, losing control. “Once operators learn a system they don’t want to give it up,” Gilbert said. What’s more, Haartz has high standards to maintain. With operations in the U.S., Mexico, Germany, India, China and Japan, changes at the headquarters plant can have a global impact.
Two things about Mahlo America gave the Haartz decision makers the encouragement they needed. “Although the system had all the bells and whistles a process engineer craves, the Windows Embedded-based interface is very intuitive,” Gilbert notes. “It’s so simple, our production crews took over after just 10 or 15 minutes of training. “Second, and probably most important, every person we met and spoke with at Mahlo knew their system thoroughly. And they totally understood our processes and challenges.”
Haartz installed its first Mahlo scanner in 2013 to test its performance in measuring total weight on a line producing material for nose and tire covers. As product requirements and challenges mounted, Haartz was easily able to assimilate Mahlo scanners into its other lines, measuring total weight, then film weight and laser thickness on the substrate, followed by full Auto Profile Control (APC) of the film weight. “The Mahlo APC gets up to production speed fast. Less material is wasted, and uptime maximized,” Gilbert noted. “Our crews and engineers were all in favor of the change.”
By the end of 2018. Haartz will have 15 Mahlo scanners online worldwide. “Lots of companies sell scanners that could probably meet our needs,” Gilbert states. “The real difference for us was the technical aptitude and service attitude of Mahlo’s people. Any time an issue comes up, Mahlo’s staff makes getting us back online their first priority.”
“Only twice since our first Haartz installation have we had to make an on-site service call,” notes Eric Reber, North American sales manager at Mahlo America Inc. “We have received the occasional call along the way, but these issues were addressed quickly through our TeamViewer service.”
The TeamViewer program is a secure remote-access service licensed with every Mahlo system sold. With it, users can give technicians temporary access to the control interface online in real time. This allows a technician to diagnose the system quickly and remotely. “TeamViewer can also be used to provide remote training for operators or engineers. Mahlo Telephone Support and TeamViewer service is included at no charge, around the clock, for the life of our system,” Reber notes.
Another feature on every Mahlo Auto Profile System is the die-bolt heater-failure alert. Haartz discovered that some of their legacy systems had quite a few dead die bolts and their graphs were giving them excessively averaged readings. “Mahlo systems graph in high resolution like a real-world sheet and give us an alert for any die bolt that’s not responding,” says Gilbert. “We’ve been able to reduce our scan-to-scan standard deviation to about 0.5% from greater than 2% previously. Also, seeing both the new scan and composite average on a single profile graph is a great feature.”
In addition to limiting waste in its manufacturing processes, Haartz strives to be “locally green” with its neighbors, communities and customers as one way to cut its carbon footprint. Haartz sources raw materials locally when possible, recycles TPO and PVC, and encourages carpooling. Continuous education and training, workplace safety, on-site fitness facilities and community-outreach programs are credited with keeping the average employee retention high.
“Maybe it’s a thing about family-operated companies, but we really like Mahlo’s simple, ‘Old World’ business approach.” Gilbert concluded, “Mahlo doesn't make machines in order to sell proprietary parts and service contracts. They engineer scanner systems that help support and strengthen our brand. That makes for a lasting business relationship.”
Related Content
How Much L/D Do You Really Need?
Just like selecting the extruder size and drive combination, the L/D should be carefully evaluated.
Read MoreFormulating LLDPE/LDPE Blends For Abuse–Resistant Blown Film
A new study shows how the type and amount of LDPE in blends with LLDPE affect the processing and strength/toughness properties of blown film. Data are shown for both LDPE-rich and LLDPE-rich blends.
Read MoreUnderstanding the ‘Science’ of Color
And as with all sciences, there are fundamentals that must be considered to do color right. Here’s a helpful start.
Read MoreWhy Compression Ratio is Important
Compression ratios have been pretty much standardized over the years, based on what has typically worked before. But there are quite a few variables that must be considered in order to get the optimum performance from your screw.
Read MoreRead Next
People 4.0 – How to Get Buy-In from Your Staff for Industry 4.0 Systems
Implementing a production monitoring system as the foundation of a ‘smart factory’ is about integrating people with new technology as much as it is about integrating machines and computers. Here are tips from a company that has gone through the process.
Read MoreWhy (and What) You Need to Dry
Other than polyolefins, almost every other polymer exhibits some level of polarity and therefore can absorb a certain amount of moisture from the atmosphere. Here’s a look at some of these materials, and what needs to be done to dry them.
Read MoreTroubleshooting Screw and Barrel Wear in Extrusion
Extruder screws and barrels will wear over time. If you are seeing a reduction in specific rate and higher discharge temperatures, wear is the likely culprit.
Read More