PUBLISHED: 5/28/2019

Materials: First Flame-Retardant TPE to Meet Standard for Railway Applications

Kraiburg’s new FR2 series offers both UL 94 VO at 1.5 mm wall thickness and DIN 45545-2 for railway applications. 


PUBLISHED: 5/23/2019

Additives: Masterbatch of Optimized Antiblock and Slip Combination for PE Blown Film

DuPont’s Dow Corning AMB-12235 launched at Chinaplas 2019 represents a new-generation of silicone-based masterbatch that features optimized combination of compatible additives to simplify processing, logistics. 


PUBLISHED: 5/21/2019

Materials: Two Performance PE Film Grades for Quality Flexible Packaging Debut at Chinaplas 2019

ExxonMobil had added two new grades to its family of Exceed metallocene hexene LLDPE film resins. 


PUBLISHED: 5/16/2019

Materials: Portfolio of Novel PBT Compounds Derived from rPET

SABIC’S LNP Elcrin iQ compounds aim to extend useful life of PET bottles and help reduce plastic waste.


PUBLISHED: 5/15/2019

Materials: Next-Generation TPEs for Overmolding Exhibit Superior Adhesion to Broad Range of Thermoplastics

Teknor Apex’s Monprene OM compounds boast cost and processing advantages over current TPEs.


PUBLISHED: 5/14/2019

Materials: LCPs Prove to be Material of Choice for Fine-Pitch Electrical Connectors

Two new high-flow, low-warpage LCP formulations from Sumitomo Chemical are key to achieving today’s thinner, smaller, higher-density interconnects.


PUBLISHED: 5/14/2019

Materials: High-Molecular-Weight POM

Polyplastics’ Duracon POM WW-09 boasts durability and good sliding performance.


PUBLISHED: 5/14/2019

Materials: Advanced PPA for FR Connectors in E/E Devices

BASF’s new Ultramid Advanced T2000 is touted for its combination of excellent mechanical and dielectric strength at high temperatures. 


PUBLISHED: 5/14/2019

Additives: Liquid Strengthening Additive Substantially Boosts Physical Properties of Recycled Polymers

Riverdale Global’s +Restore additive has been shown to strenghten PP, PP copolymer and HDPE regrind.


PUBLISHED: 5/8/2019

Materials: PC, ABS and Blends with Up to 50% Recycled Content for Broad Range of Applications

Star Plastics’ new ReStart product line boasts a sustainable materials solution that delivers quality parts and reduced waste.