Connect

AGGLOMERATION OF PLASTICS

The Plast-Agglomerator is a compact, fully automatic, and a proven continuous system that converts thermoplastic waste into high quality, free flowing granules, which are later used as valuable raw material in further processes.

All thermoplastic materials such as PE, PP, PS, PA, PET, PVC, ABS, XPS, PLA and composite materials of any kind, in the form of bulky film, fiber, or foam waste, can be continuously recycled with the same system. 

This PALLMANN Agglomeration process offers the unique advantage of material gentle agglomeration with minimum heat and minimum thermo-degradable damage; the material is heated up with friction heat only and is agglomerated, within a fraction of a second, right below the melting point. Furthermore, underwater cooling is not necessary.

The standard Plast-Agglomerator system consists of the following processing steps:  Pre-cut, Pneumatic conveying, Storing, Feeding, Agglomerating, Hot-melt granulating, Pneumatic Conveying, Pre-cooling, Air classifying, Transport and Cooling.

ADVANTAGES & FEATURES OF THE SYSTEM

  • Continuous process
  • Excellent free-flowing agglomerate with high bulk density
  • Material-gentle agglomeration by means of frictional heat
  • Minimum thermo-degradable damage
  • Fully automatic start from a cold condition
  • Low space requirement due to compact design
  • Fully automatic continuous operation

A Message from PALLMANN Industries, Inc.

Company Profile

Founded in 1903,  as flour millers and mill designers, and a family organization for 7 generations, PALLMANN is today a major machine manufacturer, with worldwide capabilities.

PALLMANN -  THE MOST INNOVATIVE, ENERGY EFFICIENT AND RELIABLE TECHNOLOGY FOR THE SIZE REDUCTION, PREPARATION AND RECYCLING OF ALL KINDS OF PLASTICS

 

 

PALLMANN ULTRA-GRANULATORSKnife Mills play an important role in the production and processing of plastics of any kind.

PALLMANN PULVERIZERS

PALLMANN has a worldwide reputation as the specialist in plastic pulverizing.

As Seen In Plastics Technology

PLMW Turbo-Finer

Pallmann Presents Pathway to Powder
At the company's booth, the theme is 'Pathway to Powder,' which showcases how Pallmann works within the framework of its new parent company. 

Recycling News at K 2013
New developments combine recycling and compounding in one step. Plenty of news at K in size reduction and de-labeling.

Rapid’s new 600 model

More Choices for Grinding, Shredding
Many granulators on display at the K 2007 show in Dusseldorf last October were big models—150 to 200 hp—to enable higher throughputs or reclaiming larger parts and chunks. For example, Rapid Granulator from Sweden brought out the 600 model, the largest in its “open-hearted” series, which allow fast access to all internal components. It has a 600-mm-diam. rotor, 100 mm more than the next largest size.

Quantec retrofit for traditional Buss kneaders

What to See at NPE 2006: Compounding and Mixing
Throughput capacities are going up for compounding equipment of all types.

Dime-sized mushroom

Wood-Plastic Composites: Weathering Quality Issues
Exterior wood-fiber composites like decks and rails haven't lived up to some of the early claims of long, maintenance-free life.

Deck

Beyond Decking: Wood Composites Branch Out
Extruded decking still drives the embryonic wood-filled plastics market. But injection and compression molded wood composites are coming on strong, and extruded profiles are moving toward more complex millwork shapes.

Product Categories of PALLMANN Industries, Inc.

Choppers (for Fiberglass)
Conveying Equipment (pneumatic and Mechanical)
Custom Size-reduction (Grinding) Services
Densifiers
Granulators
Knives for Granulators, Pelletizers
Pulverizers
Recycled/Reprocessed Materials--Bale or Bulk Form
Recycled/Reprocessed Materials--Ground Flake Form
Recycled/Reprocessed Materials--Pelletized Form
Scrap-reclaim Systems
Shredders, Guillotines