Extrusion

Troubleshooting Screw and Barrel Wear in Extrusion

Extruder screws and barrels will wear over time. If you are seeing a  reduction in specific rate and higher discharge temperatures, wear is the likely culprit.   

Read More
Extrusion

Looking to Run PCR on a Single Screw? Here’s What to Keep in Mind

Just drop it in and mix it up? Sorry, there’s a lot more to it than that. Here is some of what you need to consider.  

Read More

How Screw Design Can Boost Output of Single-Screw Extruders

Optimizing screw design for a lower discharge temperature has been shown to significantly increase output rate.

Read More
Extrusion

Troubleshooting Vent Flow Problems in Single-Screw Extruders

Vent flow can be a costly problem and a housekeeping nuisance. Here is some advice on how to eliminate it.  

Read More

The Right Way to Design Vents in Single-Screw Extruders

Designing vents for single-screw extruders requires understanding of polymer flow in the screw channels. Some designs are more effective than others. Here are some guidelines.

Read More
best practices

Extruder Alignment: Important, but Only Half the Equation

The other half? Aligning and supporting downstream equipment. Here are best practices.

Read More
Extrusion

Why Compression Ratio is Important

Compression ratios have been pretty much standardized over the years, based on what has typically worked before. But there are quite a few variables that must be considered in order to get the optimum performance from your screw.

Read More
Extrusion

How Much L/D Do You Really Need?

Just like selecting the extruder size and drive combination, the L/D should be carefully evaluated.

Read More
Extrusion

Take Proper Care in Feeding Your Extruder

Everything that happens in an extruder starts at the feed throat, so proper attention to that zone’s temperature pays off in quality and productivity.

Read More

Smaller Screws Impose Bigger Challenges

Very small extruder screws work just about like their larger cousins, but some critical differences make them harder to design and machine.

Read More
Shell Polymers (Real)ationships start here ad
Vacuum Tech for Plastics Manufacturers
quick mold change solutions injection molders
New Tinius Olsen VectorExtensometer testing
Improved Stainless 420 ESR
We Love Powders NPE
Blending Revolution
NPE2024: The Plastics Show
Specialist injection molding automation solutions