Published: 4/25/2011

Overfeeding Can Cause Surges, Too
Surging can be caused by feed restrictions, as covered in another column, and also by over-feeding or under-melting, discussed here.

Published: 3/26/2011

Solving Feed-Related Surging
Understanding the causes of surging can help troubleshoot and correct it.

Published: 1/28/2011

Extrusion: A Roll Is a Roll Is a Roll?
Chill rolls may looks simple and shiny, but they play a critical part in cooling and polishing film and sheet and are not all the same.

Published: 1/4/2011

Extrusion: Don’t Forget Zone ‘Zero’
Have you ever heard of zone zero?

Published: 1/4/2011

Extrusion: Reducing Energy, Part II: ‘Adiabatic’ Extrusion
The term adiabatic extrusion was very popular in the ’60s and ’70s, but has seemingly disappeared from the processing terminology of today.

Published: 1/3/2011

Extrusion: Run Your Chevy Volt with Extruder Energy Savings—Part I
The electricity saved on a large extrusion line could power a number of Chevrolet Volts.

Published: 12/25/2010

Extrusion: Start Up and Shut Down Properly
A key goal during startup and shutdown of the extruder is to prevent degradation of the polymer left in the extruder and downstream components such as screen changers, adapters, and dies.

Published: 8/1/2010

Tooling: The Science of Profile Die Balancing
In our last column, we discussed the five things profile extruders need to know about profile die design—proper land length, land-length ratio, drawdown, considerations for sensitive materials, and decompression.

Published: 8/1/2010

Extrusion: Take Care of Your Rolls So They Can Play Their Role
In the sheet extrusion business, one of your most important manufacturing assets is your cooling rolls.

Published: 7/1/2010

Your Extruder's Best Friend
That's the melt pump, and its main purpose is to precisely control output to the die.