Tooling Know-How: Five Tips on Profile Die Design
A poorly designed profile die—one that does not permit the part to be extruded with the same dimensions from run to run—coupled with a lack of understanding of the extrusion process, is a recipe for scrap generation.

Published: 12/1/2009

Tooling Know-How: Troubleshooting Defects--Part II: Hot-Runner Long Gate Vestiges
Last month, we discussed the general issues of an organized and disciplined process of troubleshooting and correcting mold defects.

Published: 11/1/2009

Troubleshooting Defects: Part I
Like the three other aspects of a typical mold clean/repair job (disassembly, cleaning, and assembly) there is usually more than one way to skin the cat of troubleshooting and correcting defects.

Published: 4/1/2009

The Eight Stages of Mold Repair
While the mold was still being disassembled, two “cleaners” began pulling tooling out of plates and putting them into buckets in preparation for a good scrubbing—and I mean a scrubbing.

Published: 3/1/2009

How to Determine Maximum Mold Cycle Counts
At my first production meeting with my new employer, I was told, “We want you to establish a preventive maintenance program that is based on maximum cycle counts for all our molds.” Then, before I could launch into an explanation of how ...

Published: 2/1/2009

Why Not Just Let ’r Leak?