Scrap Reclaim

Exploring the: Scrap Reclaim Zone

49 Results for: News

Sort by:
Published: 5/28/2020

Encina Turning Plastic Waste Into Renewable Base Chemicals and Fuels
Encina’s initial U.S. facility will implement the proprietary technology to produce the valuable renewable chemicals and can take plastic in varying conditions – from post-consumer, mixed plastics to ocean plastics.

Published: 5/21/2020

PLASTICS Names Winners of the 2020 Re|focus Leadership and People’s Choice Awards
PureCycle takes the Leadership in Innovation Award while Accredo Packaging wins the People's Choice Award.

Published: 5/11/2020

Nova Chemicals and Enerkem to Jointly Research New Advanced Recycling Catalyst Technology
Working together, the companies will research advanced recycling technology to transform hard-to-recycle municipal waste, including items such as plastics, household waste, and construction materials, into ethylene at full commercial scale.

Published: 4/28/2020

Wolfgang Steinwender Named CEO of NGR
Wolfgang Steinwender takes over as CEO; his predecessor Josef Hochreiter will devote more time to the further development of Next Generation Holding.

Published: 4/23/2020

Coperion and Aurora Kunststoffe Partner on Industrial Recycling Project
The companies detail how by using Coperion ZSK extruders, Aurora Kunststoffe is able to process industrial by-products and turns them into high-quality raw materials.

Published: 4/22/2020

Waste Solutions Provider Brightmark Announces New Growth Plan
Over the past two years, Brightmark has more than tripled the size of its staff, garnered  $150 million in equity investments in its projects, and acquired proprietary technology that aims to create a circular economy for post-use plastics.&nbs...

Published: 4/20/2020

Cumberland Granulators Works with Teel Plastics and KW Plastics to Help Meet Sustainability Goals
Cumberland Granulators division of ACS Group details the recent work they've done with Teel Plastics and KW Plastics to help them quantify the reduction of global warming potential at their plants.

Published: 4/20/2020

Butler-MacDonald Expands Capacity to Meet Increased Demand
The company says that March 2020 sales are up 10% over 2019.

Published: 4/20/2020

BASF and Security Matters Partner to Develop Plastics Traceability Technology
The proprietary technology from Security Matters seeks to improve the traceability and sorting of plastics in the value chain.

Published: 4/16/2020

Toyo Styrene Licenses Agilyx Recycling Technology in Japan
 The facility in Japan will focus on recycling post-use polystyrene back to styrene monomer.