Extrusion: Barrier Screws: Metering Section or Not?
A barrier screw without a metering section can reduce output and increase melt temperature.
A balanced design is required to get the best performance from a barrier screw. Barrier screws typically have three or four distinct sections that have somewhat different function, with each section balanced in relation to the others.
First is the solids-feeding section, followed by a compression or melting section, and then a metering section. The metering section is meant to stabilize the output and develop pressure to overcome the resistance of the die and downstream apparatus. Sometimes a fourth section (for mixing) is included in the design. Some barrier-screw designs have little or no metering section.
Instead, they are designed with a very long barrier section often followed by a mixer. That means the barrier section must assume the functions of the metering section as well. Using the barrier section to do this is inefficient if there is significant head pressure, particularly if processing a low-viscosity polymer. The barrier section is designed so that the melt passes over the barrier clearance and accumulates in a deep, narrow “melt channel.” The deep, narrow channel is necessary to meet the volume requirement to carry most if not all the melt forward, and the narrow width minimizes additional shear heating of the already melted polymer.
However, deep, narrow channels do not develop much pressure. In the event of substantial head pressure, these channels will have a large portion of backward flow (or pressure flow) that subtracts from the forward or drag flow, thereby reducing the net output. Moreover, the pressure flow results in repeated shear heating of the back-flowing polymer and an overall higher melt temperature. Of course, this won’t be a problem if there is a very low head pressure and/or if the extruder is equipped with a melt pump. Under those conditions, the requirement for pressure development in the metering section is largely eliminated, but stability may still be affected.
The accompanying illustration compares two barrier-screw designs that have identical dimensions except for the length of the barrier section. In a computer simulation, the screw with the longer barrier section (no metering section) has 9-10% less output at 100 rpm and 3500 psi head pressure with a 5 MFI PP copolymer.
The melt temperature is also higher; the backflow and the pressure stability exiting the screw has more variation because the discharge pressure from the solids and melt channels differ. The metering section provides a damping effect to stabilize any pressure variations coming from the barrier section. There can also be disadvantages in melting with too long a barrier section.
Any barrier-screw design—or any screw design for that matter—must be suited to the particular requirements of its application. One of those is the head pressure against which the screw will have to work. A barrier screw without any metering section compares well to one with a metering section at 500 psi head pressure, with the exception of stability. This will vary with melt temperature, polymer type and barrier screw design. I just did some extensive tests on a heavily-filled material and, when varying the head pressure with a valve, saw a drop in output of more than 15% at 3500 psi vs. a similar screw with an eight-turn metering section, which had only a 3-4% drop. If you use a melt pump, there is not much difference with or without metering, as the pressure is seldom above 1000 psi. But with this material, a melt pump was not an option.
ABOUT THE AUTHOR: Jim Frankland is a mechanical engineer who has been involved in all types of extrusion processing for more than 40 years.He is now president of Frankland Plastics Consulting, LLC. Contact jim.frankland@comcast.net or (724) 651-9196.
Related Content
The Importance of Melt & Mold Temperature
Molders should realize how significantly process conditions can influence the final properties of the part.
Read MoreHow to Select the Right Tool Steel for Mold Cavities
With cavity steel or alloy selection there are many variables that can dictate the best option.
Read MoreHow to Stop Flash
Flashing of a part can occur for several reasons—from variations in the process or material to tooling trouble.
Read MoreDensity & Molecular Weight in Polyethylene
This so-called 'commodity' material is actually quite complex, making selecting the right type a challenge.
Read MoreRead Next
People 4.0 – How to Get Buy-In from Your Staff for Industry 4.0 Systems
Implementing a production monitoring system as the foundation of a ‘smart factory’ is about integrating people with new technology as much as it is about integrating machines and computers. Here are tips from a company that has gone through the process.
Read MoreRecycling Partners Collaborate to Eliminate Production Scrap Waste at NPE2024
A collaboration between show organizer PLASTICS, recycler CPR and size reduction experts WEIMA and Conair will seek to recover and recycle 100% of the parts produced at the show.
Read More