Making the Circular Economy a Reality
Driven by brand owner demands and new worldwide legislation, the entire supply chain is working toward the shift to circularity, with some evidence the circular economy has already begun.
Sometimes change is big and you know right away, while other times change comes in smaller actions that will build up to a larger one. For instance, you purchase a reusable water bottle and see it’s now being made with Eastman Chemical’s Tritan Renew, which utilizes 50% recycled material.
Eastman is scheduled to start up what it calls the world’s largest molecular recycling facility in Kingsport, Tennessee. It will have capacity to divert annually more than 220,000 tons of “hard-to recycle” plastic waste from landfill and transform it into a variety of virgin-quality polymers.
“Circularity is about redesigning a value chain beginning to end and back to beginning,” says Scott Ballard, president of Eastman’s Plastics Division. “No one company or even industry can do it alone.
“Partnerships are needed not just with customers and suppliers but across different parts of society. Change is needed in regulations and policy, polymer technology, product design, consumer behavior, waste management, etc. — and all the change needs to be coordinated in a way that enables innovation.”
The Nalgene brand introduced reusable water bottles made from Eastman Chemical’s Tritan Renew material, which features 50% recycled content. Photo Credit: Eastman
Egor Dementev, senior analyst, plastics recycling at chemical and commodity consultant ICIS, says the circular economy has been one of the most powerful megatrends affecting the plastics industry over the last few years and is widely anticipated to keep building momentum in the future.
Despite a challenging 2023, Dementev wrote that production of mechanically recycled polymers is forecast to experience relatively strong growth supported by continuing consumer pressure, voluntary pledges and new legislation across the globe. For instance, the European Union has a plastics strategy which states that by 2030 all plastic packaging should be designed to be recyclable or reusable.
Many brands are targeting 2030 as the year to shift to a circular business model, and incorporating more recycled content and reusability across major product lines and packaging applications. But brand owners can’t achieve this alone — and that’s where the entire supply chain comes into play.
Adidas’ Circularity Ambitions
Adidas is one of the most recognizable brands in the world. The company has a long history of sustainable business practices, including creating products with recycled content, as well as promoting circularity and looking for ways to prolong the life of its products.
An Adidas spokesperson tells Plastics Technology that the company has steadily increased the amount of recycled and sustainable materials in its product range since 2015 when the company launched the first Adidas x Parley running shoe with recycled plastic waste from beaches and coastal regions.
“From there, we set an ambitious goal of using only recycled polyester by 2024, which we are on track to meet by the end of 2023 — one year ahead of schedule,” the spokesperson says. “This makes Adidas a pioneer when it comes to sustainability, as the share of recycled polyester worldwide is currently around 15%.”
Circular economy approaches like this require the cooperation of companies along the entire value chain, the spokesperson explains.
“To that end, as part of the European Union's ‘T-Rex’ project, we are working with partners from industry and science to formulate requirements for the political framework, infrastructure and technologies of a circular economy,” the spokesperson says.
In 2023, Adidas launched the Parley Pack, its first football boot pack to be made in part with Parley Ocean Plastic. Photo Credit: Adidas
Borealis’ Sustainability Focus
Stephan Roest, head of the Circular Economy business development at Borealis, says the company is seeing an increasing demand for products with reduced environmental and climate impact, yet with no compromise in quality or performance.
“To meet these needs, we work closely with our value chain partners, including brand owners, to develop tailor-made circular solutions,” he says. “This includes a range of drop-in solutions that make it easy to switch to more sustainable feedstock without the need for investment in new processing equipment or for costly and time-consuming reapproval processes.”
For the packaging industry segment, Borealis recently launched a new monomaterial pouch containing more than 95% PP and designed for recycling. Developed in collaboration with value chain partners — including Mitsui Chemical Group, Jindal Films, Profol and Huhtamaki — this more sustainable high-barrier packaging format offers a range of benefits for the blown- and cast-film extrusion processes, as well as for brand owners and end consumers.
“It is imperative that we approach the circularity challenge in a holistic way, and that means working with our value chain partners and other value-aligned companies and industry associations to develop integrated, scalable solutions,” Roest says. “The shift toward circularity is not going to happen overnight — it’s a journey, and one we need to take on together.”
Borealis introduced a new PP monomaterial pouch that is fully compatible for mechanical recycling of polypropylene. Photo Credit: Borealis
Wittmann’s Take on Circularity and the Granulator Market
John DePasquale, product manager of material handling and auxiliaries for Wittmann USA, says developments in sustainability are happening rapidly. He sees a continued adoption of zero-waste goals further improving recycling infrastructure and leading to processors finding innovative ways to repurpose or include recycled materials.
“Over the last five years, Wittmann has seen growth in granulator demand,” DePasquale says. “Most of this is due to the financial benefit of utilizing scrap. Some is due to a shift in type of resins used in certain applications and, of course, the introduction of new models throughout this time frame with enhanced features and benefits.”
Beyond throughput and infeed or cutting chamber size, there has been an increase in concern for regrind quality. DePasquale says that customers are looking to reduce amount of dust and fines to both alleviate maintenance requirements as well as produce regrind with a more consistent size and shape to minimize processing variations.
“Following the trends, there is growing interest in postconsumer resin due to increased awareness of environmental sustainability,” he says. “Many industries were looking for ways to incorporate recycled materials into their products, and PCR is gaining popularity in the packaging, automotive and consumer goods sectors.”
Related Content
In the Zone: Packaging
The Packaging Zone is the place to learn about the latest in customer product delivery.
Read MoreIn the Zone: Bottles
The Bottle Zone is the place to explore cutting-edge bottle and container technologies.
Read MoreRecycling Partners Collaborate to Eliminate Production Scrap Waste at NPE2024
A collaboration between show organizer PLASTICS, recycler CPR and size reduction experts WEIMA and Conair will seek to recover and recycle 100% of the parts produced at the show.
Read MoreIn the Zone: Sustainability Hub
NPE2024: Experience the latest eco-friendly innovations in the plastics industry at the Sustainability Hub.
Read MoreRead Next
People 4.0 – How to Get Buy-In from Your Staff for Industry 4.0 Systems
Implementing a production monitoring system as the foundation of a ‘smart factory’ is about integrating people with new technology as much as it is about integrating machines and computers. Here are tips from a company that has gone through the process.
Read MoreProcessor Turns to AI to Help Keep Machines Humming
At captive processor McConkey, a new generation of artificial intelligence models, highlighted by ChatGPT, is helping it wade through the shortage of skilled labor and keep its production lines churning out good parts.
Read MoreLead the Conversation, Change the Conversation
Coverage of single-use plastics can be both misleading and demoralizing. Here are 10 tips for changing the perception of the plastics industry at your company and in your community.
Read More