Spinning Straw Into Gold With Chemical Upcycling
Upcycling diverts waste by converting it to high value materials.
Recycling is a term with considerable cachet and a definition flexible enough to be applied to a wide variety of processes. Naturally, modifiers have been invented to distinguish and divide processes into various categories. The terms “upcycling” and “downcycling” denote processes that increase or decrease the value of a material.
A colorful quote from engineer Reiner Pilz (“Recycling? I call it DOWNcycling. They smash bricks, smash everything. What we need is UPcycling...”, from Salvo News 1994) is often cited as the origin, but the concept predates the interview by at least a decade. Pilz may not have hatched the term, but he exemplified it: cleverly designing custom interiors, made from architectural rubbish with minimal modification, creating high value from essentially zero.
The distinction promotes recycling activities that increase the value of the material used, and deprecates those that decrease it. Processing steps that increase value are more likely to be economically viable and more likely to supplant unsustainable production methods. Despite this, downcycling still makes up a large share of the plastic recycling industry. Mechanical recycling processes, preferred because of their low energy requirements, degrade plastics with each cycle, reducing molecular weight and therefore mechanical properties. While there are some closed loop processes out there, notably bottle-to-bottle PET recycling, most recycled plastics cannot be returned to the same or higher purpose.
California-based Novoloop has devised a means to upcycle the most common post-consumer waste plastic, increasing its value 50 to 80X. Its product is a thermoplastic polyurethane (TPU) made with recycled PE. TPU is known for its high abrasion resistance, making it ideal for applications where durability is critical, such as cell phone cases, automotive panels, and cable jacketing. In September, the Swiss running brand On announced its Cloudprime running shoe, a collaboration between multiple companies incorporating a variety of sustainable technologies. Novoloop TPU is being used to make the outsole.
On’s Cloudprime shoe features Novoloop TPU outsole, with 32% post consumer recyclate.
Photo Credit: On
Last month, I spoke with Novoloop CEO Miranda Wang at the 2022 K show in Germany.
“Jeanny (co-founder Jeanny Yao) and I were in high school when we visited a waste transfer facility. We were shocked to see the plastic waste that was not being recycled,” said Wang. Wang and Yao founded Novoloop, originally called Biocellection, in 2015 and developed the accelerated thermal oxidative decomposition (ATOD) that formed its basis.
Novoloop’s ATOD process breaks postconsumer PE down into diacid molecules. In a single step, the waste is purified, any dye is removed, and the diacid created, which is subsequently used to produce TPU. The process temperature and pressure are much lower than pyrolysis, according to Wang, and it produces a product that is structurally closer to a finished material.
“Sometimes the concept of circularity is applied too narrowly,” said Wang. “We are part of a bigger loop, like we see in nature, where recycling includes transformation. When a tomato plant breaks down, its nutrients may not become another tomato plant, they may become part of a tree. We don’t have to oversimplify the molecules by taking them back to base chemicals, which we would then have to expend energy to repolymerize.”
Further, the TPU produced from these diacid building blocks is a drop-in solution that requires no further modification by the customer. In the case of footwear, rubber pads can be replaced with thinner pieces of TPU with longer wear times thanks to the material properties. TPU is itself melt-recyclable, raising the possibility of further recycling loops enabling many lives for products made from Novoloop’s material.
Novoloop is currently using a pilot facility in California to create the TPU resin. The company plans to build and operate a new facility, to ramp up production to supply customers engaged in a variety of segments, potentially including automotive, bonding products, and sporting goods in addition to footwear.
The On Cloudprime shoe is not yet available to the public, but a small number have been manufactured and are being tested by elite distance runners.
Related Content
Impacts of Auto’s Switch to Sustainability
Of all the trends you can see at NPE2024, this one is BIG. Not only is the auto industry transitioning to electrification but there are concerted efforts to modify the materials used, especially polymers, for interior applications.
Read MoreAutomotive Awards Highlight ‘Firsts,’ Emerging Technologies
Annual SPE event recognizes sustainability as a major theme.
Read MorePEEK for Monolayer E-Motor Magnet Wire Insulation
Solvay’s KetaSpire KT-857 PEEK extrusion compound eliminates adhesion and sustainability constraints of conventional PEEK or enamel insulation processes.
Read MoreMolder Repairs Platen Holes with Threaded Inserts
Automotive molder ITW Deltar Fasteners found new life for the battered bolt holes on its machine platens with a solution that’s designed to last.
Read MoreRead Next
Beyond Prototypes: 8 Ways the Plastics Industry Is Using 3D Printing
Plastics processors are finding applications for 3D printing around the plant and across the supply chain. Here are 8 examples to look for at NPE2024.
Read MoreLead the Conversation, Change the Conversation
Coverage of single-use plastics can be both misleading and demoralizing. Here are 10 tips for changing the perception of the plastics industry at your company and in your community.
Read More