Borealis and Bockatech Showcasing Ultra-Lightweight Reusable PP Cups

Use of Borealis PP and Bockatech’s EconCore next-generation foaming technology yields thin-wall, robust and fully recyclable cups.

Share

Borealis and Bochatech technologies achieve ultralight PP containers
Photo Credit: Borealis Group and Bochatech

At K 2022, Borealis and Bockatech, inventor and licensor of the innovative EconCore plastic foaming manufacturing technology, are showcasing lightweight and ultra-lightweight reusable cups made of PP using EconCore. These robust and fully recyclable cups represent the many thin wall and reusable packaging applications that can be developed using Borealis PP resins and the next-generation EconCore foaming technology. Today’s ultra-lightweight cups made using Borealis PP and the EconCore technology platform for sustainable packaging are even lighter than many conventional single-use paper cups. Yet they boast good insulation properties, with twice the thermal barrier of PP cups with solid walls of the same weight.

Durable EconCore moldings can be microwave and dishwasher-safe. Because they are made solely of PP, they are easy to recycle once they have reached end of life after hundreds of use cycles. The EconCore technology produces durable, monomaterial molding walls with a composite skin-foam-skin structure in only seconds, and at low cost. When using the EconCore and Borealis PP, converters and brand owners reportedly benefit from: up to 50% less plastic, improved recyclability of molding and injection molded labels (IML), shorter cycle times of 5-to-7 seconds, and design freedom of shapes, colors, transparency and decorating elements. 

Said Borealis global commercial director consumer products Peter Voortmans, “With our partner Bockatech we’ve made unique progress in making thin wall and reusable packaging even more sustainable. The compatibility of the EconCore platform with a variety of PP resins enhances its appeal to our customers. Our Bornewables portfolio of circular polyolefins, and our transformational Borcycle C family of chemically-recycled grades can be used as drop-in solutions for food and non-food. In addition to that, our Borcycle M portfolio of mechanically recycled grades enables production of non-food applications. 



 

Related Content

  • How to Extrusion Blow Mold PHA/PLA Blends

    You need to pay attention to the inherent characteristics of biopolymers PHA/PLA materials when setting process parameters to realize better and more consistent outcomes.    

  • Advanced Recycling: Beyond Pyrolysis

    Consumer-product brand owners increasingly see advanced chemical recycling as a necessary complement to mechanical recycling if they are to meet ambitious goals for a circular economy in the next decade. Dozens of technology providers are developing new technologies to overcome the limitations of existing pyrolysis methods and to commercialize various alternative approaches to chemical recycling of plastics.

  • Processing Megatrends Drive New Product Developments at NPE2024

    It’s all about sustainability and the circular economy, and it will be on display in Orlando across all the major processes. But there will be plenty to see in automation, AI and machine learning as well.

Guill - World Leader in Extrusion Tooling
HAIDLMAIR NPE2024
Advantage temperature control units
New Micro Twin Screw Feeder NPE2024 - W8183
New 2024 Twin Screw Report
Plastics Recycling Latam
Go Beyond Blending
Gardner Business Media, Inc.
Shell Polymers (Real)ationships start here ad.