Dow, Circusil Collaborating on Silicone Recycling Facility

Dow and Circusil announced plans to construct a silicone recycling facility in Kentucky.

Share

Dow Chemical and Circusil announced a partnership to start a silicone recycling facility in Kentucky. This facility will recycle silicone waste streams from Dow’s U.S. operations as well as postindustrial waste streams from customers. Operations are targeted to begin in fourth quarter of 2024.

Circusil Plant Rendering Rendering of the planned Circusil facility. Photo Credit: Circusil LLC

The company describes the recycling process as “advanced recycling,” and says the recycled material will be reintroduced to silicone production.

The process involves depolymerizing silicone polymers to create monomers, which will in turn be repolymerized to polydimethylsiloxane (PDMS).

Dow projects that by recycling silicone waste streams, the company will be able to reduce the carbon footprint of PDMS by more than half when compared to virgin production. Recycling circumvents the production of silicon metal, which represents 55-65% of the traditional process for making silicones. Recycling can also reduce Scope 1 emissions (directly attributable to the company) and Scope 3 emissions (downstream from company operations) associated with incineration or landfilling of silicone materials at end-of-life. These results are pending critical review of life cycle analysis by an independent third party (per ISO 14040/44).

Dow expects the new facility in Paris, Kentucky, will enable its customers to: reduce the carbon footprint associated with disposal of silicone waste, meet growing demand for silicone polymers with recycled content, and accelerate progress toward sustainability objectives.

Our partnership with Circusil LLC to establish silicone recycling capabilities in North America marks a major stride forward in our pursuit of circularity. It reflects our ambition to lead silicone recycling at scale,” says Eric Peeters, vice president for Dow Performance Materials & Coatings. “As a global silicone manufacturer, we are actively delivering on our commitment to drive circularity aiming to achieve a closed-loop system on this extremely valuable material, while lowering the carbon footprint of silicones.”

Related Content

Shuttle Mold System
Shell Polymers (Real)ationships start here ad
Uway LLC
chemical foaming agents sheet and film extrusion
Guill - World Leader in Extrusion Tooling
New 2024 Twin Screw Report
See FasTie at NPE2024 in Smartflow Booth W3071
Special steels for reinforced plastics
Maguire Ultra