Extending the Repertoire of Blow Molded Nylon Fuel Tanks

The second blow molded monolayer nylon 6 auto fuel tank using DSM’s Akulon Fuel Lock is a plug-in hybrid – another first.

Share

DSM’s Akulon Fuel Lock is said to be the first monolayer nylon 6 fuel tank in a plug-in hybrid vehicle, Renault’s 2021-model Captur E-Tech.

DSM’s Akulon Fuel Lock is said to be the first monolayer nylon 6 fuel tank in a plug-in hybrid vehicle, Renault’s 2021-model Captur E-Tech. (Photo: DSM Engineering Plastics)


For more than a decade, monolayer blow molded nylon 6 has been an available alternative to coextruded or fluorinated HDPE for fuel tanks. DSM Engineering Plastics introduced Akulon Fuel Lock, a family of nylon 6 materials with higher barrier than standard PA6, allowing for thinner walls in monolayer tanks. It was offered initially for small-engine fuel tanks for lawnmowers, off-road vehicles, etc. Then, in 2018, Akulon Fuel Lock was used for the fuel tank of Renault’s Alpine A110 sports car. That was “the world’s first automotive fuel tank in polyamide,” according to DSM.

In connection with the recent K 2022 show in Düsseldorf, DSM announced what it calls another world’s first, and an extension of its partnership with Renault, in an Akulon Fuel Lock blow molded monolayer fuel tank for the 2021-model Captur E-Tech plug-in hybrid (PHEV). Its weight is much less than steel tanks and about the same as multilayer HDPE alternatives, but biobased Akulon Fuel Lock offers a simpler monomaterial solution without the complex additional features required by HDPE structures to prevent permeation and withstand the extended periods of internal pressure inherent in plug-in hybrids.

DSM also notes that Akulon Fuel Lock is a “drop-in solution” offering “a second life to the monolayer blow molding machines dedicated to production of the declining diesel monolayer fuel tanks.”

Related Content

Plastics Recycling Latam
ColorStream
New Tinius Olsen VectorExtensometer testing
Dri-Air
Maguire Ultra
Go Beyond Blending
Special steels for reinforced plastics
Shuttle Mold System
Shell Polymers (Real)ationships start here ad.