Exxon Adds Production of HDPE Molding Grades to Texas

HDPEs for pales and crates to be produced in Beaumont as well as Canada.  

Share

To help mitigate potential delivery delays cause by harsh weather, injection molding grades of HDPE for pails and crates are now available from ExxonMobil via its plant in Beaumont, Texas.  

“Previously, our injection molding HDPE grades were only available from the Sarnia, Canada facility, but this could be an issue during harsh Canadian winters,” says Dr. James Stern, HDPE Business Development Manager, North America & EMEAF. “Introducing dual sourcing from Sarnia and Beaumont helps overcome any potential logistical issues that may arise from harsh Canadian winters or tropical storms affecting the Gulf of Mexico.”

Grades are functionally equivalent between facilities, so they are an easy drop-in product for customers, ExxonMobil says.

“Whatever the cause of any logistical disruptions, having two supply points for a major portion of our North American injection molding HDPE grades helps provide greater assurances for customer business planning continuity,” Stern adds. “There’s nothing worse for a customer than supply disruptions and this move by our HDPE business is designed to help mitigate that.”

Related Content

  • Resin Prices Still Dropping

    This downward trajectory is expected to continue, primarily due to slowed demand, lower feedstock costs and adequate-to-ample supplies.  

  • Melt Flow Rate Testing–Part 1

    Though often criticized, MFR is a very good gauge of the relative average molecular weight of the polymer. Since molecular weight (MW) is the driving force behind performance in polymers, it turns out to be a very useful number.

  • The Fundamentals of Polyethylene – Part 1: The Basics

    You would think we’d know all there is to know about a material that was commercialized 80 years ago. Not so for polyethylene. Let’s start by brushing up on the basics.

Advantage temperature control units
New Tinius Olsen VectorExtensometer testing
Vacuum conveying powders to extruders compounding
Plastics Recycling Latam
Go Beyond Blending
New Micro Twin Screw Feeder NPE2024 - W8183
Trust the Experts - Purgex Purging Compounds
Special steels for reinforced plastics
Maguire Ultra