Seynsqo, the product of multinational chemical company Solvay’s 2023 split, announced succesSful feasibility testing for sorting PVDC packaging waste, conducted with Tomra. The purpose of the testing was to demonstrate the technical and economic feasibility of separating and sorting multicomponent plastic structures in which polyvinylidene chloride (PVDC) serves as a barrier layer.
Barrier shrink films such as those used in food packaging are related applications. Source: Syensqo
The partners developed a joint set of experiments with multilayer samples of commercial packaging waste consisting of LDPE and Syensqo’s Ixan PVDC. According to Syensqo, results show that multilayer films containing PVDC can be separated from mixed plastic waste using industrial sorting equipment to achieve clean-grade polyolefin and PVDC recycling streams.
“The overall target of this project was to challenge major industry standards which claim that multilayer PVDC films cannot be sorted out of multilayer packaging structures,” explains Federico Baruffi, global marketing manager, specialty polymers, at Syensqo. “Our experiments have demonstrated the contrary and are sending a clear message to the packaging and recycling industry that it can be done, notably with good accuracy and repeatability using existing industrial technology.”
The positive results apply to markets that are currently generating multilayer mixed plastic waste containing PVDC, such as shrink films in consumer and food packaging.
“One of the concerns in the recycling industry was the reliable identification of polymeric waste with PVDC content,” adds Marco Gregori, area sales manager at Tomra Recycling Sorting. “By combining our advanced optical and near-infrared detection systems, we managed to achieve a selectivity rate of more than 80% when sorting from postconsumer plastic mix and more than 95% when sorting from LDPE monolayer stream. This is yet another example of what today's technology, in this case our Autosort, can already do.”
Related Content
-
Avoid Four Common Traps In Granulation
Today, more than ever, granulation is an important step in the total production process. Our expert explains a few of the many common traps to avoid when thinking about granulators
-
SD Polymers: 'One-Stop Solution for Mechanical Recycling'
‘Passionate’ recycler invests in people and technology to meet commitment to innovative, sustainable solutions for its processor customers.
-
Foam-Core Multilayer Blow Molding: How It’s Done
Learn here how to take advantage of new lightweighting and recycle utilization opportunities in consumer packaging, thanks to a collaboration of leaders in microcellular foaming and multilayer head design.