Project OMNI, a collaborative research program directed by Recycleye, Valorplast and TotalEnergies, is developing a solution for mechanically recycling polypropylene (PP) food packaging back into food-contact applications. The project leverages machine learning and computer vision technology, coupled with efficient decontamination of food-grade PP from postconsumer waste.

Hands holding shredded plastic.

The Project OMNI approach to polypropylene sorting does not require changes to package design. Photo Credit: TotalEnergies

After 18 months of research, Project OMNI led to an alternative to digital and physical marking solutions, which require systemwide packaging changes. In a demonstration unit, Recycleye built and trained an AI model based on waste collected from 5 locations across France supplied and characterized by Valorplast. The AI and robotic sorting achieved a successful pick rate of 50% of the food-grade material, with greater than 95% purity. This sorting activity produced material used for further decontamination in a semi-industrial pilot based on off-the-shelf mechanical recycling technologies. TotalEnergies then produced odorless, clean rPP suitable for high-end packaging applications.

“We are extremely excited to see this successful application of our robust AI-powered sorting technology at a semi-industrial scale. This application opens the possibility of creating new markets for recycled plastics materials, ultimately changing the economics of recycling,” says Victor Dewulf, CEO at Recycleye. 

According to TotalEnergies, the developed process has demonstrated the efficient decontamination of food-grade PP waste sorted by AI and computer vision, and opens new opportunities for circularity of polypropylene packaging.

“This project not only demonstrates how cutting-edge technology can improve material circularity but also paves the way for a wider range of accessible applications for recycled polymers to serve our customers. It provides a concrete response to the challenge of managing end-of-life plastics, and fully supports our ambition of reaching 1 million tons of circular polymers,” says Nathalie Brunelle, senior vice president, polymers at TotalEnergies.

Related Content

chemical foaming agents sheet and film extrusion
Conair makes every pellet count
ArburgXworld
Vacuum conveying powders to extruders compounding
large tonnage injection molding productivity
VACUUM PUMPS
Gardner Business Media, Inc.
Trust the Experts - Purgex Purging Compounds
New Tinius Olsen VectorExtensometer testing