Total Energies Converts Feedstocks From Plastic Waste Into New Polymer at LaPorte Plant

Pyrolysis product from New Hope Energy was used to create monomer at BASF-Total Energies facility in Port Arthur, then polymerized to PP at Laporte

Share

Total Energies has converted feedstock from plastic waste into new polymer at its polypropylene plant in La Porte, Texas. According to the company, the La Porte plant will produce sustainably certified polymers suitable for a wide range of applications, including food grade packaging.

The petrochemical feedstock was provided by New Hope Energy's ISCC+ certified advanced recycling facility in Tyler, Texas. The feedstock was converted into monomer at the BASF Total Energies Petrochemicals (BTP) facility — a 60/40 joint venture between BASF and TotalEnergies based in Port Arthur, Texas — before being transformed into circular polymers at TotalEnergies' polypropylene plant in La Porte. Both the La Porte and BTP facilities received their ISCC+ certification in 2022.

Hands holding resin.

Total Energies is using feedstock from New Hope Energy’s pyrolysis operations, which is used to make monomer material at Port Arthur and polymerized at the Tyler facility. Source: Total Energies

Total Energies and New Hope Energy have signed a multiyear agreement, under which New Hope Energy will supply Total Energies with petrochemical feedstock made from plastics to produce recycled polymers. New Hope Energy uses a patented pyrolysis technology, developed in partnership with Lummus Technology, to process and convert plastic waste into pyrolysis oil, cracked gas and pitch.

New Hope Energy says it anticipates expanding the Tyler facility to a capacity of more than 420 metric ton per day (MPTD) of waste plastic by 2026. Total Energies has stated an ambition to produce one million tons of circular polymer by 2030.

“We are excited to partner with Total Energies in our mutual effort to transform plastic for a cleaner world,” says Rusty Combs, New Hope Energy CEO. “This supply agreement is an important step toward achieving New Hope’s goal of creating pyrolysis projects at a scale that will materially improve the nation's plastic recycling performance.”

Related Content

Plastics Recycling Latam
New Tinius Olsen VectorExtensometer testing
New Micro Twin Screw Feeder NPE2024 - W8183
Go Beyond Blending
Maguire Ultra
Guill - World Leader in Extrusion Tooling
large tonnage injection molding productivity
HAIDLMAIR NPE2024
Maguire Ultra