Bio-based Elastomer for Biopharmacuetical Tubing

Avient introduced its Versaflex elastomer formulated with bio-derived content.

Share

Avient Corporation announced the availability of Versaflex HC BIO, thermoplastic elastomer (TPE) with bio-based content. Developed as an alternative for biopharmaceutical tubing, the initial Versaflex HC BIO BT218 grade is formulated with nearly 40% first-generation biomass content, resulting in a lower carbon footprint than traditional options.

Laboratory setting with tubing in use.

Avient new product is aimed at tubing for pharmacuetical applications.
Photo Credit: Avient Corporation

The 71 Shore A formulation provides critical application performance such as weldability, kink resistance, and tensile strength comparable to leading medical tubing materials, including silicone and standard TPEs. The bio-derived grade offers greenhouse gas emissions at 2.35 kg CO2e / kg product, a nearly 25 percent lower cradle-to-gate product carbon footprint than Avient’s standard Versaflex HC BT218 grade. Avient’s product carbon footprint calculation method follows the ISO 14067:2018 standard and is certified by TUV Rheinland, an independent testing service company.

Certified for USP Class VI and ISO 10993, the new Versaflex HC BIO BT218 grade is manufactured in the United States with global commercial availability.

Related Content

Advantage temperature control units
Go Beyond Blending
ColorStream
Maguire Ultra
HAIDLMAIR NPE2024
Dri-Air
VACUUM PUMPS
Uway LLC
Guill - World Leader in Extrusion Tooling