Bonding, Sintering Tech Advances Metal Bonding for Mold, Die Components

NPE2024: Punch Industry USA exhibits P-Bas, intended to replace the use of 3D printers when producing mold and die components, as well as a variety of mold component supplies.

Share

Photo Credit, all images: Punch Industry USA

Punch Industry USA Inc.  is exhibiting its parent company’s bonding and sintering technology called P-Bas. P-Bas, an alternative to 3D metal printing, is used to fabricate custom conformal cooling channels for mold and die components by bonding split parts, offering an extensive compatibility with iron-based materials. Punch Industry has applied for a patent for this novel technology.

P-Bas, denoting Punch Bonding and Sintering, employs heat and pressure for metal bonding, achieving joint strength surpassing 90% of the base material. Additionally, P-Bas produces parts and cooling lines with a finer, smoother surface finish than that of 3D metal printed parts; the process includes a surface coating to reduce rust formation in the cooling lines. 

Parts that can be made using P-Bas include gate inserts for components to make plastic bottles, core pins for injection and die-cast molds, and sprues.

Customers can initiate the P-Bas ordering process by designing components with cooling channels, approving suggested split parts and receiving a quotation. Rigorous testing, encompassing bend tests for joint strength and leak tests for watertight integrity ensures the reliability of P-Bas technology.

Related Content

Vacuum conveying powders to extruders compounding
Trust the Experts - Purgex Purging Compounds
VACUUM PUMPS
ColorStream
New Tinius Olsen VectorExtensometer testing
Uway LLC
New 2024 Twin Screw Report
Inspect 100% of your plastics inline.
Guill - World Leader in Extrusion Tooling