Extruder Controls Make for More Energy Efficiency
NPE2024: Twin-screw extruders packed with features to optimize energy consumption.
Bausano’s next-generation MD 92 Nextmover twin-screw extruder comes equipped with the Multidrive system and Digital Extruder Control 4.0, both aimed at optimizing energy consumption.
Multidrive is a patented transmission system that enables the distribution of the coupling force over four shaft motors, controlled by a single static frequency converter, for constant rotation and perfect synchronism of the motors.
Bausano’s Digital Extruder Control 4.0 is a screening tool for extruder and end-of-line energy performance. It is an intuitive interface, enabling screw speed to be adjusted, temperature to be controlled and alarm thresholds to be set, even remotely, with a view to vertical integration of control technologies. In addition, the ability to customize multiple configurations and to consult, at any time, the archive of statistics, facilitates predictive and preventive maintenance activities, with positive results in terms of overall equipment effectiveness.
Bausano is also displaying the Smart Energy temperature control system, developed to keep the temperature of the processed material constant and reduce heat loss. The innovative technology applies the principles of electromagnetic induction to the extrusion process for faster and more uniform heating, guaranteeing consistent extrudate quality and efficiency, as high as 95% for net energy savings of 35%.
Related Content
-
The Importance of Barrel Heat and Melt Temperature
Barrel temperature may impact melting in the case of very small extruders running very slowly. Otherwise, melting is mainly the result of shear heating of the polymer.
-
Avoid Four Common Traps In Granulation
Today, more than ever, granulation is an important step in the total production process. Our expert explains a few of the many common traps to avoid when thinking about granulators
-
How to Effectively Reduce Costs with Smart Auxiliaries Technology
As drying, blending and conveying technologies grow more sophisticated, they offer processors great opportunities to reduce cost through better energy efficiency, smaller equipment footprints, reduced scrap and quicker changeovers. Increased throughput and better utilization of primary processing equipment and manpower are the results.