More Sustainable Two-Component Overmolding

Swedish compounders HEXPOL TPE AB and Polykemi AB have collaborated on a 2K sustainable development project for consumer products.

Share

HEXPOL TPE and Polykemi have collaborated on material combinations for multicomponent injection molding based on the resins’ properties and sustainability qualities. The companies’ goals included demonstrating the possibilities in reducing the product carbon footprint, while increasing recyclability and optimizing adhesion.

The compounders documented the cradle-to-gate Product Carbon Footprints (PCF) and Global Warming Potential (GWP) per kg of material. The PCF data shows that switching from a combination using fossil fuel based ABS from Polykemi, that is overmolded with a fossil fuel based TPE from HEXPOL TPE, to a recycled PP and TPE with bio-circular attributed content, can result in a 77% reduction in carbon dioxide emissions. The companies say this combination can also provide end-of-life and recycling compatibility advantages.

Combinations using mechanically recycled ABS with bio-circular attributed TPE were also tested, resulting in a 57% reduction in carbon dioxide emissions compared to the fully fossil-based equivalents. The TPE has bio-circular attributed content via the mass balance principle from 2nd generation feedstocks.

carbon footprint 2K overmolding

HEXPOL TPE and Polykemi have collaborated to determine maximum carbon reduction possibilities for overmolding PP with TPE.
Photo Credit: HEXPOL TPE and Polykemi

Related Content

See FasTie at NPE2024 in Smartflow Booth W3071
Inspect 100% of your plastics inline.
Uway LLC
Shell Polymers (Real)ationships start here ad
Go Beyond Blending
Shuttle Mold System
large tonnage injection molding productivity
Dri-Air
vacuum pumps