SABIC Offers Bio-based Versions of Noryl Resin Grades

Company will offer various levels of bio-based content in its polyphenylene ether (PPE) resin product grades.

Share

SABIC announced it is now offering bio-based versions of all Noryl, Flexible Noryl, Noryl GTX and Noryl PPX resin grades to help customers meet sustainability goals. The bio-based versions, formulated with polyphenylene ether (PPE) resin feedstocks certified under International Sustainability & Carbon Certification (ISCC) Plus, provide properties similar to those of fossil-based grades. Customers may select from multiple levels of bio-based content for their chosen Noryl product. The company plans to offer levels up to 90% bio-based in the future.

SABIC Headquarters

SABIC headquarters in Riyadh.
Photo Credit: SABIC

To demonstrate the feasibility of this bio-based approach, SABIC has  commercialized three popular Noryl grades; however, these example materials represent only part of the full offering. The availability of bio-based versions broadens the choice of Noryl resins beyond the company’s recently introduced post-consumer recycled (PCR)-based materials.

Example Bio-based Noryl Grades

The following bio-based products are available now.

  • Noryl NH5120BIO4 resin is suited for housings and enclosures, heating/ventilation/air conditioning (HVAC) components and photovoltaic/solar junction boxes. It is a bio-based, non-brominated/non-chlorinated flame-retardant resin with a UL flame rating of V1 at 1.5mm with no intentionally added per- and polyfluorinated substances (PFAS).
  • Noryl GFN2BIO3 resin features high strength, hydrolytic and dimensional stability, low warpage and low specific gravity. This bio-based material carries a UL746C outdoor suitability rating of F1, making it a candidate for indoor and outdoor applications in the building & construction and lawn & garden industries.
  • Noryl GTX902BIO3 resin is a bio-based PPE alloy that provides chemical resistance and paint-ability for potential use in applications such as automotive wheel covers, automotive electrical components and painted automotive trim.

Related Content

  • Why (and What) You Need to Dry

    Other than polyolefins, almost every other polymer exhibits some level of polarity and therefore can absorb a certain amount of moisture from the atmosphere. Here’s a look at some of these materials, and what needs to be done to dry them.

  • Melt Flow Rate Testing–Part 1

    Though often criticized, MFR is a very good gauge of the relative average molecular weight of the polymer. Since molecular weight (MW) is the driving force behind performance in polymers, it turns out to be a very useful number.

  • 50 Years...600 Issues...and Still Counting

    Matt Naitove marks his first half-century in plastics reporting, with a few of his favorite headlines.

Advantage temperature control units
Gardner Business Media, Inc.
Special steels for reinforced plastics
Maguire Ultra
Vacuum conveying powders to extruders compounding
New 2024 Twin Screw Report
New Micro Twin Screw Feeder NPE2024 - W8183
VACUUM PUMPS
Advantage chillers and temperature control units.