Thermoplastic Elastomers With Recycled Content for Automotive Applications

Avient announced new grades of TPE to meet demand for recycled content.

Share

Avient announced the launch of the Resound REC, thermoplastic elastomers with post-consumer recycled content. The new grades for automotive interior applications are formulated for comparable performance to traditional TPEs. The Resound REC 7310 product series meets common automotive original equipment manufacturer standards for volatile organic compounds and fogging.

Car interior.

Two new grades of TPE are meant for automotive interiors.
Photo Credit: Avient

 These initial grades in the series are 80 and 90 Shore A durometers and contain 35% or 45% PCR content from recycled food packaging. They can also be customized and injection molded or overmolded to PP, making them useful for a range of interior applications. This includes door mats/mat pockets, center console trays, front and rear trunk liners, or components for instrument panels & dashboards. They are colored black to provide consistent and comparable aesthetics to prime grades for OEM-specific blacks. Additional colors are also possible.

The product series is manufactured and available in North America.

Related Content

  • Resins & Additives for Sustainability in Vehicles, Electronics, Packaging & Medical

    Material suppliers have been stepping up with resins and additives for the ‘circular economy,’ ranging from mechanically or chemically recycled to biobased content.  

  • Compatibilizers Aid Recycling & Upcycling of Mixed Resins

    Compatibilizers are proving their worth in boosting critical properties such as impact/stiffness balance of PCR and PIR blends of polyolefins and other plastics.      

  • Advanced Recycling: Beyond Pyrolysis

    Consumer-product brand owners increasingly see advanced chemical recycling as a necessary complement to mechanical recycling if they are to meet ambitious goals for a circular economy in the next decade. Dozens of technology providers are developing new technologies to overcome the limitations of existing pyrolysis methods and to commercialize various alternative approaches to chemical recycling of plastics.

Dri-Air
large tonnage injection molding productivity
Inspect 100% of your plastics inline.
Dover Clear
HAIDLMAIR NPE2024
Guill - World Leader in Extrusion Tooling
New 2024 Twin Screw Report
Special steels for reinforced plastics
New Tinius Olsen VectorExtensometer testing