Composites Materials for FDM Printing

Materials are formulated for use on any pellet-based fused deposition modeling printer.

Share

Xenia Materials announced a new range of 3D printing materials, comprised of resins combined with fibers and additives. The materials are made for use in any pellet-based fused deposition modeling (FDM) printer, for large-scale additive manufacturing (LSAM) as well as high-precision production.

Xenia will offer materials dedicated to 3D printing based on its existing range of product families: Xecarb, Xebrid, Xelight and Xegreen. The Xecarb 3DP brand includes carbon fiber-reinforced polyetherimide (PEI), ABS and PC. Xebrid 3DP includes a glass and carbon fiber-reinforced ABS. Xelight 3DP includes a lightweight polyether block amide (PEBA), and Xegreen 3DP includes carbon fiber-reinforced PA6 and PA66.

3D Print Build

Xenia’s new line is aimed at additive manufacturing. Photo Credit: Xenia Materials

According to Xenia, the materials are recyclable and suitable for a wide range of applications and markets including industry, sport, sustainable mobility and defense.

Related Content

Maguire Ultra
See FasTie at NPE2024 in Smartflow Booth W3071
VACUUM PUMPS
Shuttle Mold System
Special steels for reinforced plastics
Inspect 100% of your plastics inline.
New Tinius Olsen VectorExtensometer testing
ArburgXworld
View of digital inspection records in OneView