Medical-Grade Antistatic Masterbatch for PE Films

Material reportedly efficiently empties powder from packaging materials.  

Share

Ampacet has introduced ProVital + Permstat, a non-migratory antistatic masterbatch specifically developed to provide immediate and permanent antistatic properties to polyolefin films used in pharmaceutical processes.

Ampacet ProVital+ Permstat, when used in the external layers of packaging films, creates a dissipative polymeric network within the bulk layer of the film, allowing the electrostatic charges accumulated on the film surface to dissipate throughout the external layer. The antistatic effect is immediate, consistent during the lifetime of the film and lasts as long as the film is in use.

Thanks to its dissipative effect, ProVital+ Permstat is said to efficiently empties powder from packaging materials, preventing some particles from remaining inside of the bag due to the static effect. In sealed bags, the use of ProVital+ Permstat eliminates the presence of static powder in the sealing area. ProVital+ Permstat can be incorporated into polyethylene cleanroom films, which are used to store and transfer pharmaceutical raw materials or active pharmaceutical ingredients used in drug production.

Antistat Masterbatch for PE Medical Films

Photo: Ampacet

ProVital+ Permstat provides full consistency of formulation with a no-change policy for raw materials at the CAS and commercial level, with manufacturing under consistent process parameters and controlled-room production to minimize cross contamination risks.

Related Content

  • The Effects of Stress on Polymers

    Previously we have discussed the effects of temperature and time on the long-term behavior of polymers. Now let's take a look at stress.

  • The Strain Rate Effect

    The rate of loading for a plastic material is a key component of how we perceive its performance. 

  • Melt Flow Rate Testing–Part 1

    Though often criticized, MFR is a very good gauge of the relative average molecular weight of the polymer. Since molecular weight (MW) is the driving force behind performance in polymers, it turns out to be a very useful number.

ColorStream
See FasTie at NPE2024 in Smartflow Booth W3071
Guill - World Leader in Extrusion Tooling
Shell Polymers (Real)ationships start here ad
Dri-Air
Maguire Ultra
Go Beyond Blending
Shuttle Mold System
HAIDLMAIR NPE2024