MATERIALS: High-Performance TPVs from New Source
WEB EXCLUSIVE: Alliance Polymers and Services LLC, Romulus, Mich., has launched a second series of its own TPVs, weeks after it introduced its first series of Viprene G general-purpose TPVs.
WEB EXCLUSIVE: Alliance Polymers and Services LLC, Romulus, Mich., has launched a second series of its own TPVs, weeks after it introduced its first series of Viprene G general-purpose TPVs (see January’s Keeping Up With Technology section online). New Viprene P is a series of high-performance TPVs available with a high compression-set resistance for rugged applications, and in a wide range of hardnesses from 45 Shore A to 50 Shore D. Suggested applications include power steering, brake, and fuel hoses; bellows; under-hood components; appliances; and electrical, construction, and industrial parts.