Materials: Low-Warpage, High Hydrolysis-Resistant PBT for Automotive
Polyplastics’ Duranex flame-retardant PBT boasts outstanding electrical properties plus high rigidity and low warpage.
The Polyplastics Group (U.S. office in Farmingdale, Mich., has launched new Duranex PBT that has the outstanding electrical properties traditionally found in PBT, while also offering other important performance attributes. Duranex 750AM is a 30% glass-reinforced, flame-retardant (FR) grade with low warpage, high rigidity, and heat and moisture resistance (hydrolysis resistance). It is said to be ideally suited for automotive applications such as communications devices and high-pressure parts for electric vehicles (EVs) and hybrid electric vehicles (HEVs).
Until now, it has been difficult to satisfy requirements for both flame resistance and hydrolysis resistance because hydrolysis resistance typically decreases with the addition of a FR component. There has been an increasing demand for FR materials in the automotive market for use in communication devices and high-pressure parts for EVs and HEVs. These materials must also meet the auto industry’s need for high durability and outstanding formability. Duranex 750AM and other PBTs also meet the demands of electrical and electronics applications.
Polyplastics can produce low-warpage PBT materials such as Duranex 750AM via three methods. First, the anisotropy of the shrinkage rate can be reduced by using spherical and plate-like fillers with low aspect ratios rather than fiber fillers. This reduces warpage, but can also adversely affect mechanical strength.
Second, the absolute value of the shrinkage rate can be reduced by forming alloys with amorphous resins such as PC and SAN. This method results in a small reduction in mechanical strength, while the amorphous resin also has an effect on thermal properties and other factors. Third, improving flowability and reducing pressure distribution (shrinkage rate distribution) inside the cavity can reduce warpage, though not as much as the aforementioned two methods.
Related Content
-
Getting into Plastics Additive Manufacturing? Avoid these Six Common Errors
There are a lot of 3D printing technologies out there, and it’s not uncommon for processors new to additive manufacturing to get tripped up. Here are some typical snafus, along with advice on how to avoid them before you start making parts.
-
Additive Fusion Technology Optimizes Composite Structures for Demanding Applications
9T Labs continues to enhance the efficiency of its technology, which produces composite parts with intentionally oriented fibers.
-
Make Every Shot Count: Mold Simulation Maximizes Functional Parts From Printed Tooling
If a printed tool only has a finite number of shots in it, why waste any of them on process development?