Clear, Anti-Fogging PP Lid for Microwaveable Food Packaging
Milliken’s clarifier help food packaging thermoformer convert from OPS to clarified PP.
A clear, anti-fogging PP lid for microwaveable food packaging developed by Taiwan’s South Plastic Industry Co. Ltd. (SPI), a leading Asian manufacturer of thermoformed plastic food packaging, in collaboration with Milliken &Co., has replaced oriented polystyrene (OPS). Many suppliers use OPS for their ready-meal packaging lids, but those can only withstand 185 F/85 C temperatures and are not suitable for microwaveable products.
SPI has been striving for years to do this but had not found a way to get PP to meet all performance requirements while also retaining the clarity and non-yellowing aesthetics that are key to consumer appeal. By leveraging on its close, five-year relationship with Milliken, SPI finally achieved its goals. To produce the UltraClear PP resin, the collaborators used Milliken’s Millad NX 8000 clarifier that has been shown to deliver on all the required performance along with processing benefits.
According to SPI president Tosho Wang, by using Milliken’s additives, which also include Hyperform HPN performance nucleating agent in its PP formulations, SPI is now able to thermoform its products at a lower processing temperature, which reduces their energy usage. Moreover, these additives allow SPI to produce a thinner PP lid without affecting rigidity, which in turn helps to reduce plastic usage while increasing output.
SPI, which now uses Milliken clarifiers in all its UltraClear PP packaging products, says it plans to explore using the material to expand the use of PP in more food applications, including some that currently use PET.
Related Content
-
Resins & Additives for Sustainability in Vehicles, Electronics, Packaging & Medical
Material suppliers have been stepping up with resins and additives for the ‘circular economy,’ ranging from mechanically or chemically recycled to biobased content.
-
K 2022 Additives & Materials: Sustainability in the Lead
Nearly all of the new additives highlighted at the big show are aimed at enhancing recyclability of commodity resins and some volume engineering resins such as nylon and PC. A few new materials, on which we had not previously reported, also surfaced at K 2022.
-
PFAS-Free Processing Aid for Blown Film Extrusion
Ampacet’s new processing aid said to perform as well as fluoro-based PPAs in blown film.