Printable Thermoset Polyurethane
Chromatic 3D Materials launched ChromaMotive D65, designed for additive manufacturing.
Chromatic 3D Materials announced the launch of its ChromaMotive D65. ChromaMotive D65 is a rigid thermoset polyurethane formulated for reactive extrusion additive manufacturing with the company’s RX-AM platform.
One application of the thermoset polyurethane is for sports equipment including ski boots, where impact resistance at low temperatures is desirable. Photo Credit: Chromatic 3D
According to the company, the new material performs well in a range of extreme cold to elevated temperatures from -30˚C up to 120˚C, and has mechanical properties comparable to injection-molded TPU, HDPE and PP. ChromaMotive D65 is compatible with Chromatic’s RX-Flow printers, which are suitable for development work and low- to medium-volume industrial production.
In addition to winter sports gear, potential applications include parts for the aerospace, automotive and agricultural industries with varying temperature requirements.
“With ChromaMotive D65, manufacturers that are producing rigid plastic components can take advantage of RX-AM’s fast print speeds and the ability to print on textiles, plastics and
metals. Now it’s possible to 3D print rigid parts at industrial volumes for everything from winter recreational equipment to aircraft interiors,” says Cora Leibig, Chromatic founder and CEO.
Chromatic will be demonstrating 3D printed parts made from ChromaMotive and its other material offerings at the International Elastomer Conference being held this week in Cleveland.
Related Content
-
Large-Format “Cold” 3D Printing With Polypropylene and Polyethylene
Israeli startup Largix has developed a production solution that can 3D print PP and PE without melting them. Its first test? Custom tanks for chemical storage.
-
How Additive Manufacturing Can Help, not Hinder, Injection Moldability of New Designs
Four cost drivers—design for moldability, mold-base size, internal componentry, polish/custom finishing—dictate the financial and processing success of a molded part design. Learn how 3D printing can assist this process, while also understanding its potential pitfalls.
-
Daimler, OMIC Evaluate Wire-Fed DED for Moldmaking
3D printing a core and cavity on machine from Gefertec, followed by machining, allowed for a complete mold tool to be produced in three days.