MATERIALS: Biobased Blends for Home Compostable, Low-Gauge Films
FKuR's new Bio-Flex blends used in grocery bags that biodegrade completely in garden compost.

Published: 9/15/2016

MATERIALS: Biobased Blends for Thinner Compostable Films
FKuR to showcase the first of it compostable compounds based on new technology for packaging films with particularly low thickness and puncture resistance.

Published: 4/18/2016

MATERIALS: Biobased BOPET Film for Solar Control Windows
Toray Plastics launches energy-saving solar protection film made with sustainable feedstock.

Published: 4/15/2016

MATERIALS: DSM’s Biobased Polymer Portfolio Expands with Nylon 4T Grades
Aimed at thinner and more sustainable electronic devices, the new grades boast an improved processing window.

Published: 3/11/2016

TESTING: Thermal Analysis Tester Elevates Performance and Efficiency
TA Instruments' new DSC systems have enhanced sensing technologies for thermal analysis of polymers and biomaterials.

Published: 2/8/2016

ADDITIVES: Expanded Availability of Amorphous PHA for Enhancing PVC and PLA
Metabolix's new line of a-PHA grades serve as performance additives for PVC, PLA.

Published: 8/6/2015

MATERIALS: Partially Biobased PP Compound for Injection Molding
What appears to be the first commercially available partially biobased PP compound is newly available from FKuR.

Published: 7/7/2015

MATERIALS: Bioplastic 3D Filament with Exceptional Finish
One-year old 3Dom USA is offering a new plant-based filament that offers several advantages.

Published: 5/10/2015

MATERIALS: High-Performance PLA For Durables Rivals ABS
NatureWorks' new ABS replacement formulations are indicative of the continued evolution of Ingeo PLA resins.

Published: 1/28/2015

MATERIALS: Fine-Ground Cellulosic Filler Used in Renewable Compounds
Microscopic cellulose particles enhance properties and renewable content.