Additives for Boosting Performance and Sustainability of PE and PP Packaging

NPE 2024: Milliken’s UltraGuard 2.0 boosts barrier performance in HDPE and LLDPE while Hyperform HPN 58ei  improves properties of PP FDA-approved sheet and thermoformed packaging.  

Share

Milliken launches additives that boost performance of PE and PP packaging
Source: Milliken

Two new additive masterbatches for polyolefins that offer both improved performance and sustainability benefits are newly available from Milliken.

  • UltraGuard 2.0 builds on Milliken’s long-standing line of tailored masterbatches for PE to improve barrier performance in HDPE and LLDPE by up to 70% — subsequently supporting more monomaterial packaging options and material downgauging.
     
  • Hyperform HPN 58ei enhances performance for PP sheets and thermoformed parts to deliver improved optical performance, isotropic shrinkage and regrind quality, and is FDA approved for food packaging.

Milliken works across the value chain to enable PP and PE formulations that make plastics more reusable, recyclable and efficient without sacrificing performance. With a range of clarifier and nucleator agents, masterbatches, polymeric colorants, and viscosity and performance modifiers, Milliken’s portfolio helps its customers and brand owners achieve their own sustainability goals.

Complementing its overarching approach to responsible manufacturing processes and in alignment with the company’s 2025 sustainability goals and its near- and long-term net-zero targets, Milliken develops products that support its customers’ sustainability goals, says Milliken’s Global Vice President for plastic additives Wim Van de Velde.


 

NPE 2024

Milliken & Company will be exhibiting new technology at NPE 2024 in Orlando, FL this May.


Plan to meet up with their team or get registered here!

Related Content

Gardner Business Media, Inc.
TracerVM Flow Meter features many display options
Guill - World Leader in Extrusion Tooling
New Tinius Olsen VectorExtensometer testing
Orbetron new for 2024 micro twin screw feeder
Bole Machinery
Vacuum Tech for Plastics Manufacturers
Trust the experts for fast & efficient changeovers
Cranes, Conveyors, Racks, Loaders, Accessories