International Space Station Now 3D Printing with PEI/PC Materials
PEI/PC compound is the third material a developer of zero-gravity 3D printers has demonstrated on the International Space Station for space-based additive manufacturing.
U.S.-based Made In Space, a developer of zero-gravity 3D printers and an official supplier to NASA, recently announced it has begun using PEI/PC (polyetherimide/polycarbonate) blends, a high-performance alloy, for 3D printing in its Additive Manufacturing Facility (AMF) aboard the International Space Station (ISS). PEI/PC is an aerospace-grade polymer that produces stronger, more heat-resistant materials. Blends of PEI/PC, such as ULTEM 9085 and ULTEM 1010, are used in additive manufacturing in the commercial aerospace industry.
“Made In Space is proud to add PEI/PC to the suite of materials it is manufacturing in space with,” MIS President & CEO Andrew Rush said. “Our team has been regularly printing parts in space with AMF for over a year now. This unparalleled knowledge base of in-space manufacturing operations will enable us to deliver future in-space manufacturing solutions in the most cost effective and efficient ways possible.”
Last year, I reported that MIS worked with Braskem to produce green PE specifically for 3D printing in zero gravity. The technology allows astronauts to fabricate tools and spare parts in space using the biobased resin.
Terrestrially, PEI/PC is used in aircraft cabins and in the medical industry. Having nearly triple the tensile strength of ABS, a high strength-to-weight ratio and low off-gassing properties, PEI/PC has been used in space on external hardware and satellites. According to Rush:
“Manufacturing in PEI/PC really expands the value of in-space manufacturing for human spaceflight. PEI/PC is a truly space-capable material. With it, extra-vehicular activity (EVA) tools and repairs, stronger and more capable intra-vehicular activity (IVA) tools, spares, and repairs, and even satellite structure can be created on site, on demand. That enables safer, less mass-intensive missions and scientific experiments.”
Up Next: Making Parts for Space, In Space
One program PEI/PC will benefit is the Archinaut Development Program, which MIS has contracted with NASA on. Archinaut is a platform that manufactures, assembles, and integrates space-optimized systems. These systems include reflectors, antennae, trusses, booms, and radiators. Archinaut is specifically designed to create large structures for space, in space. In its basic configuration, Archinaut is a system integrated into a satellite and includes a space-capable manufacturing unit, assembly robotics, feedstock, and prefabricated components. Once in orbit, space-optimized structures are manufactured and integrated into the satellite which can be larger, more capable, and/or lighter than traditional deployables can achieve.
Archinaut is specifically designed to create large structures for space, in space.
Related Content
-
Make Every Shot Count: Mold Simulation Maximizes Functional Parts From Printed Tooling
If a printed tool only has a finite number of shots in it, why waste any of them on process development?
-
Medical Manufacturer Innovates with Additive Manufacturing and Extrusion Technology Hubs
Spectrum Plastics Group offers customers two technology hubs — one for extrusion, the other for additive manufacturing — to help bring ground-breaking products to market faster.
-
Getting into Plastics Additive Manufacturing? Avoid these Six Common Errors
There are a lot of 3D printing technologies out there, and it’s not uncommon for processors new to additive manufacturing to get tripped up. Here are some typical snafus, along with advice on how to avoid them before you start making parts.