PE Flat, PP Moving Up; PS, PVC, PET Flat-to-Down
Resin and monomer production disruptions halted further price decreases, but there’s still downward potential.
Prices of key feedstocks for the five commodity resins overall continue to be lower in June, but unplanned and planned production outages resulted in prices bottoming out for PE and PP. A reversal in pricing was being attempted for the two polyolefins, though that’s only likely to happen for PP. Meanwhile, prices for PET dropped a bit more, with similar expectations for both PS and PVC in the July/August timeframe.
These are the views of purchasing consultants from Resin Technology, Inc. (RTi), Fort Worth, Texas, CEO Michael Greenberg of Plastics Exchange, The, Chicago, and Houston-based PetroChemWire (PCW).
PE PRICES FLAT
Polyethylene prices remained flat through June, following a price reduction of generally 3¢/lb by some suppliers, according to Mike Burns, RTi’s v.p. of client services for PE. Suppliers were out with a 3¢/lb hike for July, but Burns expected all PE prices to remain flat through July and August, noting that a PE price change in the July-August time frame took place just once in a span of 10 years.
An expected earlier scenario of further resin decreases is not materializing, primarily due to several unplanned and planned production disruptions, which tightened the market. Moreover, recovery of suppliers’ inventories did not take place as originally thought, this while domestic demand continues to be rather robust, said Burns. PCW reported that spot supply was relatively balanced because of robust domestic demand and production outages. They noted that HDPE pressure pipe and conduit sales in particular have seen strong growth this year, contribution to the healthy demand overall.
Both Burns and PCW characterized export markets as quiet, partly due to lack of material and slowed demand. Interestingly, PE suppliers have been running plants in the high 80s-to-low-90s%, versus mid-to-high 90s during the last few years.
The Plastic Exchange’s Greenberg described the spot market as ho-hum, noting that processors had a negative outlook on pricing—which had dropped some and then stabilized—and were buying smaller sized orders. Also, he noted that many processors claimed to have been well supplied through July.
Commenting on current domestic prices, Burns noted, “The reality is that pricing is now good—ideal delta with Chinese PE prices is 7-10¢/lb and we are now at 8¢/lb. Meanwhile, Dow expected to start up its now LLDPE production this month and CP Chem is expected to start up its new HDPE and LLDPE production in third quarter.
PP PRICE FLAT-TO-UP
Polypropylene prices were flat in June, in step with propylene monomer, which rolled over from May at 38.5¢/lb, However, production disruptions at two PDH on-purpose propylene units resulted in monomer tightness. July monomer contract nominations stood at 2-3¢/lb and PP suppliers were poised to issue similar resin price hikes, according to Scott Newell, RTi’s v.p. of PP markets.
Burns noted that LBI issued a price increase expansion margin of 3¢ on top of the monomer increase, effective this month, but there was no further industry support. The Plastics Exchange’s Greenberg reported, “We believe the market is now settling up for another series of margin expanding increases ahead, though the success would not be an automatic slam dunk.” Factors that could influence this trend is the slow but steady demand in downstream demand with no new resin production complexes on the near horizon—essentially tipping supply/ demand in favor of PP suppliers.
Demand for PP was very good in May and June, following the drop in prices--a total of 13.5¢/lb in April/May time frame, so buyers were stocking up, according to Newell. Unplanned production outages for both PP and PP impact copolymer tightened things up.
PCW described PP spot prices a flat- to-higher due to the tighter supply. Still, Greenberg described PP trading activity as improving, with buyers becoming a bid more aggressive with their orders and spot demand showing signs of strengthening. Spot PP homopolymer remained available, but prices have ticked up a few cents, while PP copolymer had become scarce and commanded a growing premium. PCW also reported on Braskem’s late June announcement that it will construct a 962 million lb/yr plant adjacent to existing PP units in LaPorte, Texas, with an expected startup in first quarter 2020. The
“Delta” line represents Braskem’s seventh production line in the U.S., and will produce homopolymers, random copolymers, impact copolymers and reactor thermoplastic polyolefins.
PS PRICES FLAT
Polystyrene prices remained flat in June, following a cumulative 7¢/lb drop in the two previous months, and due to a rollover in benzene contract prices, according to Mark Kallman, RTi’s v.p. of client services for engineering resins, PS, and PVC.PCW reported spot PS prices were flat-to-lower amid seasonally slower demand. Spot styrene monomer at end of June, ended up down by 9%. Spot benzene slid nearly 20 ¢/gal. Kallman ventured that July benzene contract prices would settled down 10-20¢/gal. This could trans- late to a July decrease of 1-2¢/lb for PS resins.
Meanwhile, PCW reported that spot prime general-purpose PS remained flat while generic prime HIPS was down 1¢/ lb as global butadiene prices plunged. Kallman concedes that there is an “unusual” pressure from imports—more specifically, for prime HIPS imports from the Far East and Brazil, which are coming into port at 64¢/lb. Following repackaging and transport, that price moves up by 10¢/lb but is still attractively priced compared to domestic prime HIPS.
PVC PRICES FLAT-TO-DOWN
PVC prices remained flat in June, but and had good potential for dropping between 1-2¢/lb in the July-August timeframe, according to RTi’s Kallman. This driven primarily by ample supplies of ethylene and lower spot prices through June, which would result in lower July ethylene contract settlements, as well as lower crude oil prices.
Meanwhile, domestic demand for PVC through May, was up 2% year-to-date. PVC production has recovered to January levels, so suppliers’ inventories are in much better shape. For now, exports are flat-to-down.
PET PRICES DOWN
Domestic bottle-grade prime PET prices in June averaged 55.5¢/lb, down 2.2¢/lb from May, based on PCW’s Daily PET Report. That price represents PET business on a delivered Chicago basis. The price on June 30, dropped to 54¢/lb, driven primarily by lower costs of raw materials PTA, MEG and PX.
Meanwhile, prices of imported prime PET, with an IV of 78 ml/gram or higher, also fell in June, averaging 51.4¢/lb, down 2.5¢ from May. This represented PET resin on a delivered duty-paid U.S. port basis. The price for imported PET on June 30, was 53.5¢/lb. PET feedstock costs in June averaged 50.5¢/lb, down 1.31c/lb from May, according to a calculation used to price prime PET for monthly invoicing by resin suppliers and distributors supplying domestic end users.
Related Content
In Sustainable Packaging, the Word is ‘Monomaterial’
In both flexible and rigid packaging, the trend is to replace multimaterial laminates, coextrusions and “composites” with single-material structures, usually based on PE or PP. Nonpackaging applications are following suit.
Read MorePrices Up for PE, PP, PS, Flat for PVC, PET
Trajectory is generally flat-to-down for all commodity resins.
Read MoreFundamentals of Polyethylene – Part 6: PE Performance
Don’t assume you know everything there is to know about PE because it’s been around so long. Here is yet another example of how the performance of PE is influenced by molecular weight and density.
Read MoreMelt Flow Rate Testing–Part 1
Though often criticized, MFR is a very good gauge of the relative average molecular weight of the polymer. Since molecular weight (MW) is the driving force behind performance in polymers, it turns out to be a very useful number.
Read MoreRead Next
Most Resin Prices Down or Flat; PC and Nylon 66 Up for Now
Falling feedstock prices are a key driver as we enter the third quarter.
Read MorePeople 4.0 – How to Get Buy-In from Your Staff for Industry 4.0 Systems
Implementing a production monitoring system as the foundation of a ‘smart factory’ is about integrating people with new technology as much as it is about integrating machines and computers. Here are tips from a company that has gone through the process.
Read MoreHow Polymer Melts in Single-Screw Extruders
Understanding how polymer melts in a single-screw extruder could help you optimize your screw design to eliminate defect-causing solid polymer fragments.
Read More