First Automotive Plastic Parts from Mixed Automotive Plastic Waste
LyondellBasell and Audi collaborate on creating seatbelt buckle covers for the 2023 Audi Q8 e-tron
A first-time collaboration to help close the loop for mixed automotive plastic waste has been underway between polyolefins manufacturer LyondellBasell and Audi. For the 2023 Audi e-tron luxury SUV and its coupe-shaped Sportback sibling, Audi is installing plastic seatbelt buckle covers made using LyondellBasell plastic that supports the sourcing of feedstocks from mixed automotive plastic waste. Plastic components from customer vehicles that can no longer be repaired are dismantled, shredded, and processed by chemical recycling into pyrolysis oil.
The pyrolysis oil is then used as a raw material in LyondellBasell’s manufacturing process for the production of new plastics, replacing virgin fossil feedstocks. The recycled content is attributed to the Audi product via a mass balance approach. Said new business development director Erik Licht at LyondellBasell Advanced Polymer Solutions, “As part of the PlasticLoop project, we are working with Audi to establish an innovative closed-loop process, recycling plastic automotive parts for use in new vehicles. For the first time, we are using chemical recycling to recycle mixed automotive plastic waste into plastic granulate for automotive interior applications.”
With this process, LyondellBasell, Audi, and chemical recycler SynCycle (Next Generation Group and BDI), succeed in recycling a stream of material which today is mostly only suitable for energy recovery. This reduces the usage of fossil-based primary materials for the Audi Q8 e-tron and keeps valuable feedstocks in a circular loop. Materials produced from pyrolysis oil reportedly are of the same high quality as virgin materials and have the same properties. Chemical recycling offers an alternative to energy recovery and complements mechanical recycling.
Related Content
-
Celanese to ‘Shine’ at CES 2023 with Expanded Portfolio of Materials
With it acquisition of DuPont’s engineering resins, Celanese’s resin solutions for automotive electrification, e-mobility and consumer electronics are plentiful.
-
Impacts of Auto’s Switch to Sustainability
Of all the trends you'll see at NPE2024, this one is BIG. Not only is the auto industry transitioning to electrification but there are concerted efforts to modify the materials used, especially polymers, for interior applications.
-
Design Optimization Software Finds Weight-Saving Solutions Outside the Traditional Realm
Resin supplier Celanese turned to startup Rafinex and its Möbius software to optimize the design for an engine bracket, ultimately reducing weight by 25% while maintaining mechanical performance and function.