A new coupling agent and compatibilizer is specially designed for natural fi bers in polypropylene. Licocene PP MA 6452 TP is the newest addition to a novel line of maleic anhydride-grafted olefi n waxes made with metallocene catalysts from Clariant Corp.’s Pigments & Additives Div., Coventry, R.I. This additive is based on PP wax. It replaces Clariant’s Licomont AR 504 wax produced with conventional catalysis. Tel: (704) 331-7000 • www.clariant.com