Published

Level Your Press in an Hour or Less

Injection Molding Know How

A level injection molding machine is necessary to keep producing high-quality parts. Here's how to do it right.

Share

Your injection molding machine is leveled on installation, but how long does it take for it to drift out of level? How often should it be checked or re-leveled? For that matter, why bother leveling it in the first place? Isn’t the machine’s frame strong enough to keep things aligned?

Unfortunately, regardless of age, your machines need to be level to keep the platen parallel and the parting line of the mold in good shape—in other words to keep producing consistent, high-quality parts.

Let’s start with why the machine needs to be level. Upon clamp-up, the mold halves must mate perfectly and clamp evenly to keep the platen parallel and prevent flash, parting-line wear, and mold damage. If the machine is not level, the two halves of the mold will actually grind a wee bit on clamping, as they mate and reach tonnage. In fact, there will be a twisting motion as the two halves mate, and you’ll get parting-line wear. When the parting line wears and/or vents get peened shut, you’ll get flash, cosmetic blemishes, and/or burns on the part. Parting lines wear in normal production, but a machine that’s not properly leveled will accelerate the issue.

Part problems caused by an out-of-level machine often are not seen right away and are misdiagnosed when they are observed. Most processors will assume they are having an issue with the mold. They’ll bring the mold to the tool shop for redressing the parting line or for some other repair, only to put it back in the press and see the same part problems before the first or second production run is completed.

Do we agree now that it’s wise to have the machine level? OK, then how do we get it there…the first time? Usually it’s done this way: Someone places a machinist’s level across the tiebars near the stationary platen, and then levels the machine. Then the level is moved near the die-height platen, and the leveling feet are adjusted once more. Then the level may be placed parallel on a tiebar, with the leveling feet once again adjusted. Then each leveling position is rechecked, only to find that more leveling is needed. This approach can take hours, and still not yield the desired result.

Try another method: First, round up three machinist’s levels (yes, three), one torque wrench, and two people.

My suggestion is to buy a torque wrench and just one of the levels you’ll need. These things are expensive and most of the time just sit around. Try to find two other molders nearby with levels and borrow them when needed (and of course share yours).

Here’s my method:

1. Go to each leveling foot and clean and oil each of the leveling screws.

2. Of the two persons assigned to this task, pick the one with the most mechanical ability. Give him or her the torque wrench and get each of the leveling feet at the same torque. I wish I could tell you what number to shoot for but it varies with the type of leveling foot, weight of the machine, etc. The main idea is to get each foot to support about the same amount of weight. One needs a bit of mechanical sense to find the number for each machine/location. You might be surprised how level the machine is at this point.

3. Place one level across the tiebars (or guide ways, if they are supporting the platen), against the stationary platen. Place another level near the die-height adjustment platen, and the third parallel along one of the tiebars.

4. The person in the best position to see all three levels should now instruct the one who did the initial adjustment which feet to slowly move up or down until all three levels are level.

5. This will take 30 to 45 min, though big machines take a bit longer. Move on to the next machine on the list.

How often should this be done? I suggest at least once a year. There is no readout on the computer screen to provide information on the machine level; you have to get maintenance to check this

Related Content

PBT and PET Polyester: The Difference Crystallinity Makes

To properly understand the differences in performance between PET and PBT we need to compare apples to apples—the semi-crystalline forms of each polymer.

Read More
screws

How Much L/D Do You Really Need?

Just like selecting the extruder size and drive combination, the L/D should be carefully evaluated.

Read More
pet

Why (and What) You Need to Dry

Other than polyolefins, almost every other polymer exhibits some level of polarity and therefore can absorb a certain amount of moisture from the atmosphere. Here’s a look at some of these materials, and what needs to be done to dry them.

Read More
Commodity Resins

Density & Molecular Weight in Polyethylene

This so-called 'commodity' material is actually quite complex, making selecting the right type a challenge.

Read More

Read Next

Extrusion Know How

Troubleshooting Screw and Barrel Wear in Extrusion

Extruder screws and barrels will wear over time. If you are seeing a  reduction in specific rate and higher discharge temperatures, wear is the likely culprit.   

Read More
processing tips

People 4.0 – How to Get Buy-In from Your Staff for Industry 4.0 Systems

Implementing a production monitoring system as the foundation of a ‘smart factory’ is about integrating people with new technology as much as it is about integrating machines and computers. Here are tips from a company that has gone through the process.

Read More
Extrusion

Understanding Melting in Single-Screw Extruders

You can better visualize the melting process by “flipping” the observation point so that the barrel appears to be turning clockwise around a stationary screw.

Read More