Custom molder ITW Deltar Fasteners, Chippewa Falls, Wis., faced a unique challenge with a high-volume acetal fastener. Achieving a quality surface finish required using faster injection speeds, but those speeds also pushed pressures higher in what was already a pressure-limited process.

“It seemed that anything we tried to do to reduce the pressure—open the sprue, open up the runner, increase the temperature—would have a negative impact to the cycle,” explains Brock Cooley, tooling engineer at ITW Deltar Fasteners. “So we had to try to find that fine line and balance to achieve the optimum process.”

Cooley posed this process challenge to Scott Wahl of mold-component supplier PCS Company, Fraser, Mich., and Wahl saw an opportunity to pitch a new product borne of a new collaboration. PCS had recently begun working with Jason Murphy, president of Next Chapter Manufacturing (NXCMFG; Grand Rapids, Mich.) a toolmaker that applies additive manufacturing technologies. PCS was working with NXCMFG on mold components that utilize 3D printing, and one of the first developments to come from that partnership was a sprue bushing featuring a conformal cooling channel.

That product, which comes in 10 sizes, features a patent-pending design that maximizes the surface area of a 1/8-in. water line. Squeezed into a “kidney shape,” according to Murphy, the cooling line forms a sort of double helix that wraps all the way around the sprue bushing, crossing at the top before coming back down and exiting at the bottom, with one water inlet and one outlet. The component is formed from H13 steel via direct metal laser sintering.

“Because it is a 1/8-in. water line it enables a higher level of flow,” Murphy says, “contrary to smaller, more restrictive lines.”

Prior to applying the conformally cooled sprue bushing, the eight-cavity fastener tool was running a 20.3-sec cycle at 22,500 psi. When the first iteration of the new sprue bushing was installed, those numbers dropped to 17.8 sec and 22,000 psi. When a duplicate mold for the part was made, a new sprue bushing was created and by tweaking the orifice size, the molder dropped the cycle time to 15.7 sec with a pressure of about 18,000 psi. “What the new bushing did was allow us to increase our nozzle size on the press but still have the sprue set up in time,” Cooley explains.

PCS and NXCMFG see big opportunities for the new sprue-bushing concept, especially where large sprues meet multiple small cavities.

“When you have small parts and multiple cavities,” Murphy says, “you have to start out with a very large sprue so that by the time you step down to the smallest cavities, you’re feeding them properly. With a larger sprue and small parts, your sprue is going to be the limiting factor in cycle time.”

Related Content

Vacuum Tech for Plastics Manufacturers
Trust the experts for fast & efficient changeovers
Dover Clear
Go Beyond Blending
TracerVM Flow Meter features many display options
Plastics Recycling Latam
Improved Stainless 420 ESR
quick mold change solutions injection molders
Guill - World Leader in Extrusion Tooling