rPlanet Earth Opens Vertically Integrated Recycling Plant In California
Among a range of reclaim and polymer processing systems in place at the Vernon plant are three Welex sheet lines supplied by Graham Engineering Corp. and equipped with EDI extrusion dies and BKG melt delivery components from Nordson Corp.
rPlanet Earth, a new company dedicated to closed-loop recycling of post-consumer plastics, has started up a large grassroots facility that the company calls the “world’s first” completely vertically integrated plant for converting PET packaging waste into finished rPET products with properties reportedly comparable to those made from virgin PET.
The 302,000 sq.ft facility in Vernon, Calif., takes in bottles, clamshell containers, and other packaging waste from curbside collection; puts it through an extensive series of sorting and cleaning procedures; grinds it into flake and subjects it to rigorous wash and decontamination; raises the intrinsic viscosity (IV) of the material in accordance with end-use requirements; and processes it into food-grade sheet, thermoformed containers, and injection molded preforms for bottles. The new rPlanet Earth plant has an annual capacity of 80 million lb.
The total investment at Vernon thus far is over $100 million. According to rPlanet Earth co-CEO Robert Daviduk, plans are in the works to add a second bales-to-end-product production line in the facility within the next two years. “The utilities and other infrastructure are already in place to support a new line that can have a capacity 50% larger than that of our existing line,” says Daviduk. “Our company has plans to build three or more new plants at sites elsewhere in the U.S. and possibly in other countries.”
Beyond recycling PET, rPlanet Earth meets other sustainability goals, noted co-CEO Joseph Ross. “While our rPET packaging provides appearance, purity and physical properties comparable to those of virgin PET, our carbon footprint is 60% less than that of packaging made from virgin resin and in fact is 20% less than that for rPET products from other companies,” says Ross. He added that the figures take into account curbside collection, baling, and transportation as well as the operation in the Vernon plant. “In addition, our recycling operation uses 90% less water, per quantity of output, than a PET resin plant.”
Among a range of reclaim and polymer processing systems in place at the Vernon plant are three Welex sheet lines supplied by Graham Engineering Corp., York, Pa., and equipped with EDI extrusion dies and BKG melt delivery components from Nordson Corp., Westlake, Ohio.
THE PROCESS
After bales entering the rPlanet Earth facility have been broken into a single stream of bottles and thermoforms, the material is subjected to multiple sorting procedures. Magnetized sorters remove foreign matter such as wire; near-infrared scanners identify PET and separate it from other polymers; and another sorting step separates PET materials by color. Next comes a dry system for grinding the material into flake; water is avoided because it is a carrier for inks and adhesives that can negatively affect the quality of the finished rPET. The first encounter with water is in the wash line, where the material is cleaned before it moves to a tank where PET, which is heavier than water, sinks, while labels, adhesives, and other matter are skimmed off. Subsequently the flake enters a Krones (U.S. office in Franklin, Wis.)MetaPure reactor where ~200 °C heat and vacuum are used in a final decontamination process; solid state polymerization (SSP) raises the IV of the rPET to various levels, depending on the target application.
rPlanet Earth bypasses the pelletizing step in favor of adding value to flake by using it in its own in-house plastics processing lines. “By skipping the pelletizing of rPET we potentially avoid degrading our products’ appearance, since a melting step that can negatively affect color is completely eliminated,” Daviduk says. “Our customers are looking for products that come from a truly closed-loop recycling system.” He noted that rPlanet Earth can supply sheet, thermoformed packaging, or preforms whose rPET content can range up to 100%, depending on whether or not a customer requires some percentage of virgin PET.
The company currently operates seven plastics processing lines: Two Husky, Bolton, Ontario, Canada, injection molding systems are for production of preforms; and three Welex, York, Pa., extrusion lines produce sheet for sale as rollstock to the merchant market or for use in-house on two large Lyle thermoforming machines. The thermoformed products manufactured by rPlanet Earth may include drinking cups, produce packaging, clamshell containers, and virtually any other food-grade thermoformed packaging currently made from PET.
The three Welex sheet lines supplied by Graham engineering include extruders that yield widths up to 75 in. and can be configured for coextrusion; XSL Navigator controls capable of integrating with plant-wide automation systems; Nordson’s BKG HiCon screen changers, BlueFlow gear pumps, and static mixers; and Nordson’s EDI Ultraflex sheet dies. Graham Engineering also supplied thickness scanners, edge trim systems, winders, and other equipment.
“We spent an enormous amount of time researching plastics processing equipment suppliers and chose Graham Engineering because of their technical capabilities, their engineering and design support, and their Converge CTS [Conical Twin Screw] technology, which is more compact and streamlined in comparison with conventional twin-screw systems,” Ross says. “It was a joint decision between us and Graham Engineering to include Nordson components. The in-line backflush capability of the BKG screen changers was particularly attractive because this self-cleaning feature enables us to avoid shutdowns due to screen buildup. In addition, Nordson backed their EDI die with extensive experience in PET sheet processing, exceeding that of other die suppliers.”
Related Content
Advanced Recycling: Beyond Pyrolysis
Consumer-product brand owners increasingly see advanced chemical recycling as a necessary complement to mechanical recycling if they are to meet ambitious goals for a circular economy in the next decade. Dozens of technology providers are developing new technologies to overcome the limitations of existing pyrolysis methods and to commercialize various alternative approaches to chemical recycling of plastics.
Read MoreHow to Optimize Injection Molding of PHA and PHA/PLA Blends
Here are processing guidelines aimed at both getting the PHA resin into the process without degrading it, and reducing residence time at melt temperatures.
Read MoreFilm Extrusion: Boost Mechanical Properties and Rate of Composting by Blending Amorphous PHA into PLA
A unique amorphous PHA has been shown to enhance the mechanical performance and accelerate the biodegradation of other compostable polymers PLA in blown film.
Read MoreAvoid Four Common Traps In Granulation
Today, more than ever, granulation is an important step in the total production process. Our expert explains a few of the many common traps to avoid when thinking about granulators
Read MoreRead Next
Advanced Recycling: Beyond Pyrolysis
Consumer-product brand owners increasingly see advanced chemical recycling as a necessary complement to mechanical recycling if they are to meet ambitious goals for a circular economy in the next decade. Dozens of technology providers are developing new technologies to overcome the limitations of existing pyrolysis methods and to commercialize various alternative approaches to chemical recycling of plastics.
Read MoreWhy (and What) You Need to Dry
Other than polyolefins, almost every other polymer exhibits some level of polarity and therefore can absorb a certain amount of moisture from the atmosphere. Here’s a look at some of these materials, and what needs to be done to dry them.
Read More